daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Effect of Deformation Temperature on Microstructure and Properties of Gradient Extrusion of TB8 Titanium Alloy AITranslate

School of Materials Science and Engineering,Hefei University of Technology;School of Materials Science and Engineering,Hefei University of Technology;School of Materials Science and Engineering,Hefei University of Technology;School of Materials Science and Engineering,Hefei University of Technology;School of Materials Science and Engineering,Hefei University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

To study the influence role of deformation temperature on the gradient microstructure and pro-perties of TB8 titanium alloy,gradient extrusion tests were conducted on TB8 titanium alloy at 850℃,900℃and 950℃,and the variation laws of microstructure and microhardness of specimens at different deformation temperatures were investigated by OM and XRD.The experimental results show that after gradient extrusion,the specimen can be divided into three deformation zones,including the core micro-defor-mation zone,the sub-center medium deformation zone,and the edge large deformation zone,showing a gradient distribution of the grain size gradually decreasing from the core to the edge.After the gradient extrusion and deformation,the sub-grain size of the material decreases while its microscopic strain and dislocation density increase significantly;decreasing the deformation temperature can significantly refine the grains and increase the overall hardness value.The hardness of the specimen edge at 850℃increases by 16.32%compared with that of the core.

KeyWords AITranslate

deformation temperature gradient extrusion gradient microstructure hardness dislocation density TB8 titanium alloy

1徐铁伟,李金山,张丰收,王飞云,刘向宏,冯勇.TB8钛合金冷变形过程的组织演变及其热处理时效响应(英文)[J].稀有金属材料与工程,2016,45(3):575-580. 被引量:8

2唐波,唐斌,韩逢博,李金山,杨冠军.TB8钛合金β相变点附近高温变形行为研究(英文)[J].稀有金属材料与工程,2013,42(9):1761-1766. 被引量:8

3赵波,姜燕,别文博.超声滚压技术在表面强化中的研究与应用进展[J].航空学报,2020,41(10):37-62. 被引量:17

4薛克敏,周金朝,郭胜华,闫中原,张勇强,李萍.难变形Ti_(2)AlNb基合金梯度挤压工艺数值模拟和试验研究[J].塑性工程学报,2022,29(7):1-10. 被引量:1

5李萍,段园培,张青,王锋,薛克敏.基于摩擦修正的TB8合金热压缩流变应力行为分析[J].稀有金属,2009,33(2):137-141. 被引量:12

6薛克敏,段园培,李萍,张青.TB8钛合金的热变形行为及加工图[J].材料工程,2007,35(z1):57-60. 被引量:8

7张青,李萍,薛克敏.TB8合金再结晶组织的分形特征[J].材料研究与应用,2011,5(1):31-34. 被引量:6

8张坤,董洪波,姜智勇,石尚,刘洪骁.冷变形及时效工艺对TB8钛合金组织及性能影响的研究[J].稀有金属,2019,43(9):904-910. 被引量:6

9Dan Liu,Daoxin Liu,Mario Guagliano,Xingchen Xu,Kaifa Fan,Sara Bagherifard.Contribution of ultrasonic surface rolling process to the fatigue properties of TB8 alloy with body-centered cubic structure[J].材料科学技术:英文版,2021(2):63-74. 被引量:5

10邹忠波,董洪波,王明主,王鑫.双道次热变形工艺参数对TB8钛合金显微组织的影响[J].特种铸造及有色合金,2016,36(7):751-754. 被引量:2

1王雯雯,王宇斌,田家怡,雷大士,桂婉婷.电解水对生石膏超细磨的影响及作用机理[J].矿产保护与利用,2022,42(6):159-166.

2孙启坤,王鹏,李良,冯富春,张新意,黄荣.基于内聚力模型的动力电池胶粘连接仿真研究[J].时代汽车,2023(14):115-118.

3王硕,林军,吴涛,侯帅,霍纯森,王广春.超声微锻造辅助定向能量沉积316L不锈钢 微观组织与力学性能研究[J].精密成形工程,2023,15(7):20-28.

4徐刚.挤压比对Mg-9Gd-4Y-2Zn-0.5Zr合金组织和力学性能影响[J].热加工工艺,2023,52(7):103-105.

5赵颖,王俊霖,运新兵,郭丽丽,闫志勇,张旭.大应变条件下铝锶中间合金连续挤压组织演变[J].稀有金属材料与工程,2023,52(3):1094-1102.

6王周头,袁清,张庆枭,刘升,徐光.冷轧中碳梯度马氏体钢的组织与力学性能[J].金属学报,2023,59(6):821-828.

7桂婉婷,雷大士,王宇斌,王雯雯,田晓珍.外磁场及硫酸镁对碳酸钙溶解行为的影响机理研究[J].化工矿物与加工,2023,52(6):1-5.

8马乐.利用化学实验测试手段对自来水中微量有机污染物的检测与分析研究[J].中国科技期刊数据库 工业A,2023(5):0188-0191.

9罗开广,吴雨泽,熊汉青,张昀,Charlie KONG,喻海良.采用深冷异步轧制提高高熵合金颗粒增强铝基复合材料的力学性能[J].中国有色金属学报:英文版,2023,33(7):1988-2000.

10张瑞,梅大江,石小兔,张庆礼,马荣国,张俊蕊,窦仁勤,孙贵花,王小飞,张德明,高进云.YAG晶体位错密度分布及蚀坑形貌[J].硅酸盐学报,2023,51(6):1396-1405.

Basic Information:

DOI:

Chinese Library Classification Number:TG379[金属学及工艺—金属压力加工]

Citation Information:

To study the influence role of deformation temperature on the gradient microstructure and pro-perties of TB8 titanium alloy,gradient extrusion tests were conducted on TB8 titanium alloy at 850℃,900℃and 950℃,and the variation laws of microstructure and microhardness of specimens at different deformation temperatures were investigated by OM and XRD.The experimental results show that after gradient extrusion,the specimen can be divided into three deformation zones,including the core micro-defor-mation zone,the sub-center medium deformation zone,and the edge large deformation zone,showing a gradient distribution of the grain size gradually decreasing from the core to the edge.After the gradient extrusion and deformation,the sub-grain size of the material decreases while its microscopic strain and dislocation density increase significantly;decreasing the deformation temperature can significantly refine the grains and increase the overall hardness value.The hardness of the specimen edge at 850℃increases by 16.32%compared with that of the core.

quote

GB/T 7714-2015 [1] LI Ping, ZHANG Yue, HUANG Xiao-yu, et al. Effect of Deformation Temperature on Microstructure and Properties of Gradient Extrusion of TB8 Titanium Alloy[J]. Rare Metals and Cemented Carbides, 2023(3): 70-76.
MLA [1] LI Ping, et al., "Effect of Deformation Temperature on Microstructure and Properties of Gradient Extrusion of TB8 Titanium Alloy." Rare Metals and Cemented Carbides, no. 3, 2023, pp. 70-76.
APA [1] LI Ping, ZHANG Yue, HUANG Xiao-yu, GUO Sheng-hua, & XUE Ke-min. (2023). Effect of Deformation Temperature on Microstructure and Properties of Gradient Extrusion of TB8 Titanium Alloy. Rare Metals and Cemented Carbides(3), 70-76.
IEEE [1] LI Ping, ZHANG Yue, HUANG Xiao-yu, GUO Sheng-hua, and XUE Ke-min, "Effect of Deformation Temperature on Microstructure and Properties of Gradient Extrusion of TB8 Titanium Alloy," Rare Metals and Cemented Carbides, no. 3, pp. 70-76, 2023. keywords: {deformation temperature;gradient extrusion;gradient microstructure;hardness;dislocation density;TB8 titanium alloy}