Thermal Separation and Recycling of Lithium Iron Phosphate Cathode Waste AITranslate
Abstract AITranslate
Problems in the conventional recycling process of lithium iron phosphate cathode waste include huge resource consumption,tedious steps,and secondary pollution.Using absolute ethanol as the solvent,lithium iron phosphate cathode waste was thermally dissolved to achieve the non-destructive and effective separation of the active substance from the current collector,and the phase structure and electrochemical properties of the regenerated LiFePO_4 cathode material at different calcination temperatures were characterized.The results show that the regenerated LiFePO_4 cathode materials obtained by calcination at diffe-rent temperatures have a pure phase,and the cathode material obtained by pre-calcination at 450°C for 4 h followed by calcination at 650°C for 10 h shows the maximum diffraction intensity.The constant-current charge/discharge test results at room temperature in 2.5~4.3 V voltage range show that the cathode material calcined at 650°C for 10 h exhibits the maximum discharge specific capacity of 137.8 mA·h/g,a capacity retention rate of 92.8%after 100 cycles,and a Coulombic efficiency close to 99%.The electrochemical impedance spectroscopy of this cathode material also exhibits a minimum charge transfer impe-dance of 130Ω.The absolute ethanol thermal dissolution method also provides a new separation way for the recovery of similar materials.
KeyWords AITranslate
1曾诗涵,张继享,吴燕芳,杨净,钱庆荣,陈庆华,曾令兴.退役动力电池磷酸铁锂正极材料的应用现状和回收利用技术[J].再生资源与循环经济,2022,15(3):28-32. 被引量:7
2陈永珍,黎华玲,宋文吉,涂小琳,冯自平.废旧磷酸铁锂电池回收技术研究进展[J].储能科学与技术,2019,8(2):237-247. 被引量:33
3叶焕英.废旧磷酸铁锂电池的回收再生概述[J].皮革制作与环保科技,2021,2(18):111-112. 被引量:1
4靳星,贾美丽,杜浩,郑诗礼,张懿,王少娜,李兴彬,魏昶.废旧磷酸铁锂正极材料回收再生研究进展[J].有色金属工程,2020,10(11):64-72. 被引量:27
5赵红伟,施志聪(指导).废旧磷酸铁锂电池正极材料回收技术进展[J].电池工业,2021,25(5):271-278. 被引量:5
6伍德佑,刘志强,饶帅,张魁芳.废旧磷酸铁锂电池正极材料回收利用技术的研究进展[J].有色金属:冶炼部分,2020(10):70-78. 被引量:22
7鲍维东,骆艳华,裴晓东.废旧磷酸铁锂锂离子电池正极的回收[J].电池,2020,50(2):200-203. 被引量:14
8刘进龙.磷酸铁锂废旧电池的回收概况[J].石油化工安全环保技术,2019,35(4):64-66. 被引量:12
9王百年,王宇,刘京,杨保俊,张娟.废旧磷酸铁锂电池中锂元素的回收技术[J].电源技术,2019,43(1):57-59. 被引量:13
10伍德佑,王东兴,刘志强,饶帅,张魁芳.氧压硫酸浸出废旧磷酸铁锂电池选择性回收锂[J].中国有色金属学报:英文版,2022,32(6):2071-2079. 被引量:2
1陈建,庞志强,卢宪芹,吉海瑞,董翠华.锂盐体系中生物质高效转化及利用研究进展[J].生物质化学工程,2023,57(4):71-78.
2徐莺歌,王世伟,梁补女,毛生红,孔令斌.VS_(4)/rGO纳米复合材料的制备及储钠性能研究[J].真空与低温,2023,29(4):348-355.
3吴鑫,李存玉,邓祥敏,牛敏,华政颖.绿原酸与生物碱配伍后成分存在状态与超滤膜传质行为的相关性研究[J].中成药,2023,45(6):1960-1963.
4Qingya Guo,Fanglin Xu,Lin Shen,Shungui Deng,Zhiyan Wang,Mengqi Li,Xiayin Yao.20μm-Thick Li_(6.4)La_(3)Zr_(1.4)Ta_(0.6)O_(12)-Based Flexible Solid Electrolytes for All-Solid-State Lithium Batteries[J].能源材料前沿(英文),2022(1):206-213.
5余雷,王瑞娟,田俐,阳立.3D集流体在锂金属电池中的应用研究进展[J].人工晶体学报,2023,52(6):1086-1099.
6徐欢,夏章讯,景粉宁,王素力,孙公权.重整气组分对HT-PEMFC性能影响研究[J].电源技术,2023,47(6):687-692.
7尹才洪,张泽磊.一种改性纳米SiO_(2)/聚合物复合材料涂层的制备[J].装备制造与教育,2023,37(2):50-53.
8徐瑞瑶,黄沥,黄兴民,赵君文,韩靖.Cr含量对TiB_(2)/FeCr基复合材料显微组织和高温氧化行为的影响[J].钛工业进展,2023,40(3):19-27.
9王泽,唐淑璟,李素华,张可翔,彭洪亮,闫二虎,孙立贤.Al_(2)O_(3)/LiAlO_(2)表面包覆改性LiNi_(1/3)Co_(1/3)Mn_(1/3)O_(2)三元正极材料研究[J].聊城大学学报:自然科学版,2023,36(3):56-63.
10曾帅波,陈烨,唐俊雄,潘惜园,彭静,郑浩荣,李涌仪,伍强,徐伟.基于三元、磷酸铁锂和锰酸锂正极的电化学性能比较[J].广东技术师范大学学报,2023,44(3):53-58.
Basic Information:
DOI:
Chinese Library Classification Number:TF09[冶金工程—冶金物理化学]
Citation Information:
Problems in the conventional recycling process of lithium iron phosphate cathode waste include huge resource consumption,tedious steps,and secondary pollution.Using absolute ethanol as the solvent,lithium iron phosphate cathode waste was thermally dissolved to achieve the non-destructive and effective separation of the active substance from the current collector,and the phase structure and electrochemical properties of the regenerated LiFePO_4 cathode material at different calcination temperatures were characterized.The results show that the regenerated LiFePO_4 cathode materials obtained by calcination at diffe-rent temperatures have a pure phase,and the cathode material obtained by pre-calcination at 450°C for 4 h followed by calcination at 650°C for 10 h shows the maximum diffraction intensity.The constant-current charge/discharge test results at room temperature in 2.5~4.3 V voltage range show that the cathode material calcined at 650°C for 10 h exhibits the maximum discharge specific capacity of 137.8 mA·h/g,a capacity retention rate of 92.8%after 100 cycles,and a Coulombic efficiency close to 99%.The electrochemical impedance spectroscopy of this cathode material also exhibits a minimum charge transfer impe-dance of 130Ω.The absolute ethanol thermal dissolution method also provides a new separation way for the recovery of similar materials.
quote
| GB/T 7714-2015 | [1] ZHANG Yu-cai. Thermal Separation and Recycling of Lithium Iron Phosphate Cathode Waste[J]. Rare Metals and Cemented Carbides, 2023(3): 82-86. |
| MLA | [1] ZHANG Yu-cai. "Thermal Separation and Recycling of Lithium Iron Phosphate Cathode Waste." Rare Metals and Cemented Carbides, no. 3, 2023, pp. 82-86. |
| APA | [1] ZHANG Yu-cai. (2023). Thermal Separation and Recycling of Lithium Iron Phosphate Cathode Waste. Rare Metals and Cemented Carbides(3), 82-86. |
| IEEE | [1] ZHANG Yu-cai, "Thermal Separation and Recycling of Lithium Iron Phosphate Cathode Waste," Rare Metals and Cemented Carbides, no. 3, pp. 82-86, 2023. keywords: {lithium-ion battery;LiFePO4;cathode waste recovery;green solvent;cyclic voltammetry} |