Research on Friction and Wear Behavior of Nano-La_2O_3 Doped Mo_2NiB_2 -based Cermets AITranslate
Abstract AITranslate
Using Ni-6 B-53.3 Mo as basic materials,Mo2NiB2-based cermets with different La2O3 doping concentration(0%,0.3%,0.6%,0.9%,1.2%)were prepared by vacuum hot-pressed sintering at 970℃.The effects of La2O3 doping concentration on the microstructure and friction and wear properties of Mo2NiB2-based cermets were investigated by high temperature vacuum friction and wear tester,surface profiler,laser confocal microscopy and X-ray diffraction.The results show that with the increase of La2O3 content,the wear rate and friction coeffiction of Mo2NiB2-based cermets are increased first and then decreased under the same load at room temperature.The wear rate and friction coefficient of Mo2NiB2-based cermets doped with 0.3%La2O3 are the highest and doped with 1.2%La2O3 are the lowest.The effects of load on wear resistance of Mo2NiB2-based cermets is obvious,the wear rate and friction coeffiction decrease with the increase of load.As temperature increases,the wear rate of La2O3 doped Mo2NiB2-based cermets decreases first and then stabilizes gradually,and the friction coefficient decreases first and then increases.
KeyWords AITranslate
1童幸生,张静.氧化铝陶瓷摩擦磨损实验研究[J].江汉大学学报:自然科学版,2011,39(2):34-37. 被引量:8
2承新,郑勇,于海军,卜海建,严永林,赵能伟.三元硼化物基金属陶瓷的研究进展[J].材料导报,2007,21(7):52-54. 被引量:18
3代宽宽,宋光明,吴钱林,李文戈.Mo-Ni-B系三元硼化物陶瓷涂层激光熔覆制备及其腐蚀性能[J].腐蚀与防护,2012,33(5):375-377. 被引量:8
4杨林,潘应君,柯德庆,徐源源,王盼.稀土Sm_2O_3对Mo_2NiB_2基金属陶瓷微观组织和力学性能的影响[J].武汉科技大学学报,2017,40(2):105-109. 被引量:9
5钟培金.Mo含量对含Mn和V的Mo_2NiB_2基硬质合金显微结构和机械性能的影响[J].稀有金属快报,2004(10):41-41. 被引量:1
1郭世柏,易正翼,段晓云,郭涛,龚望.载荷和速率对(W,Mo)C/Al2O3/La2O3材料高温摩擦磨损性能的影响[J].稀有金属,2020,44(10):1029-1036. 被引量:4
2李强,李文戈,赵远涛,王争强,袁东林,张淼.Mo2NiB2基金属陶瓷制备技术及应用的研究进展[J].机械工程材料,2020,44(10):12-16. 被引量:2
3倪晓杰,开佳伟,尹莉,赵忠贤,赵远涛,王生泽,胡肇炜,李文戈.船舶维修与再制造用Mo_(2)NiB_(2)基金属陶瓷及涂层的制备和研究现状[J].机械工程材料,2021,45(5):8-14. 被引量:2
1刘庆生,程华金,郭浩,王学重,高帅涛.钨晶体生长的数值模拟与晶习预测[J].稀有金属,2021,45(7):848-856.
2樊战博,李文虎,艾桃桃,董洪峰,张良,余明.热压烧结无粘结相Mo_(2)NiB_(2)金属陶瓷的制备及性能[J].材料热处理学报,2021,42(11):155-161.
3开佳伟,尹莉,胡肇炜,赵远涛,李文戈.激光熔覆Mo_(2)NiB_(2)熔覆层温度场与应力场仿真研究[J].陶瓷学报,2021,42(6):1064-1071. 被引量:2
4马玉康,侯清宇,黄贞益,光剑锋,马啸宇,伍厚玲.含铜钼基合金涂层的SPS烧结及组织性能[J].稀有金属,2022,46(2):153-161. 被引量:1
5叶平元,钱东升,王华君,蒋骋,姚振华.H13钢基自润滑模具材料组织与性能[J].塑性工程学报,2022,29(10):230-236.
6邓伟涛,李文戈,张杨杨,张博文,张士陶,赵远涛.粉末球磨时间对Mo2NiB2金属陶瓷组织与性能的影响[J].机械工程材料,2022,46(11):20-25.
7王雨馨,董艳春,姜洁,刘佳宁,田芸,陈景柏,杨勇,何继宁.等离子反应合成Ni60B-TiN梯度涂层的组织与性能[J].表面技术,2023,52(4):138-146.
8邱殿强,苏暄博,王喆,武笑宇,谢述锋.表面防护技术在舰船维修领域中的应用研究进展[J].材料开发与应用,2023,38(2):91-96.
1专利名称:一种镍基合金作粘结相的Mo2NiB2基金属陶瓷及其制备方法[J].中国钼业,2019,43(1):28-28.
2杨尚余,邢学刚,张娇娇,王昊,司马林,王鹤峰.稀土氧化物掺杂对氧化铝陶瓷力学性能和摩擦磨损性能的影响[J].功能材料,2018,49(6):190-195. 被引量:7
3庞秋,胡志力,谷万里,吉国强,孙东立.CNTs含量对CNTs/Al微观组织及力学性能的影响[J].材料科学与工艺,2019,27(1):30-38.
4严仙荣,李晓杰,王小红,闫鸿浩.硼掺杂纳米金刚石的制备及表征(英文)[J].稀有金属材料与工程,2018,47(12):3634-3639. 被引量:2
5唐伟,刘志研,李耀,廖佩珊,马睿.杂化壳聚糖气凝胶的制备及其疏水改性[J].科技创新与应用,2019,9(15):10-11. 被引量:2
6齐东丽,宋健宇,沈龙海.N_2气流量比对磁控溅射Mo-N涂层结构和性能的影响[J].表面技术,2019,48(2):173-178. 被引量:1
7童庆,陈泉志,莫秋凤,董婉冰,蒋智秋,李伟洲.预置Ti粉对激光氮化TC4涂层组织及性能的影响[J].中国表面工程,2018,31(5):167-174. 被引量:1
8方双全,田郭涛,秦云晴,翁辉.层状陶瓷Ti_3AlC_2的制备与腐蚀行为[J].材料热处理学报,2019,40(3):168-172. 被引量:2
9何帅,孙德恩,曾宪光,王建川.钨与钒掺杂类金刚石薄膜的温度适应摩擦磨损机制研究[J].化工新型材料,2019,47(4):162-166. 被引量:3
10王少青,吴向清,谢发勤.占空比对TiAl合金表面阴极微弧沉积Al_2O_3涂层的影响研究[J].表面技术,2019,48(2):232-238.
Basic Information:
DOI:
Chinese Library Classification Number:TG148[金属学及工艺—金属材料]
Citation Information:
Using Ni-6 B-53.3 Mo as basic materials,Mo2NiB2-based cermets with different La2O3 doping concentration(0%,0.3%,0.6%,0.9%,1.2%)were prepared by vacuum hot-pressed sintering at 970℃.The effects of La2O3 doping concentration on the microstructure and friction and wear properties of Mo2NiB2-based cermets were investigated by high temperature vacuum friction and wear tester,surface profiler,laser confocal microscopy and X-ray diffraction.The results show that with the increase of La2O3 content,the wear rate and friction coeffiction of Mo2NiB2-based cermets are increased first and then decreased under the same load at room temperature.The wear rate and friction coefficient of Mo2NiB2-based cermets doped with 0.3%La2O3 are the highest and doped with 1.2%La2O3 are the lowest.The effects of load on wear resistance of Mo2NiB2-based cermets is obvious,the wear rate and friction coeffiction decrease with the increase of load.As temperature increases,the wear rate of La2O3 doped Mo2NiB2-based cermets decreases first and then stabilizes gradually,and the friction coefficient decreases first and then increases.
quote
| GB/T 7714-2015 | [1] ZHOU Pei-de, LI Wen-hu, AI Tao-tao, et al. Research on Friction and Wear Behavior of Nano-La_2O_3 Doped Mo_2NiB_2 -based Cermets[J]. Rare Metals and Cemented Carbides, 2019(2): 10-14. |
| MLA | [1] ZHOU Pei-de, et al., "Research on Friction and Wear Behavior of Nano-La_2O_3 Doped Mo_2NiB_2 -based Cermets." Rare Metals and Cemented Carbides, no. 2, 2019, pp. 10-14. |
| APA | [1] ZHOU Pei-de, LI Wen-hu, AI Tao-tao, NIU Qun-fei, & ZHANG Liang. (2019). Research on Friction and Wear Behavior of Nano-La_2O_3 Doped Mo_2NiB_2 -based Cermets. Rare Metals and Cemented Carbides(2), 10-14. |
| IEEE | [1] ZHOU Pei-de, LI Wen-hu, AI Tao-tao, NIU Qun-fei, and ZHANG Liang, "Research on Friction and Wear Behavior of Nano-La_2O_3 Doped Mo_2NiB_2 -based Cermets," Rare Metals and Cemented Carbides, no. 2, pp. 10-14, 2019. keywords: {La2O3 doping;Mo2NiB2-based cermets;microstructure;friction and wear properties} |