Study on Oxidation Behavior and Protective Measures of TaW12 Alloy during Forging Process AITranslate

Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The oxide layer thickness and oxidation products during the forging process of TaW12 alloy were characterized by optical microscopy and XRD technology,and the macro-oxidation behavior were investigated.The results show that during unprotected forging,the surface of the alloy absorbs a lot of oxygen,resulting in seriously powdered surface and harden sub-surface,with the oxidation depth of about 300~400μm,and the oxidation product is Ta2O5.The oxidation of the alloy could be greatly reduced by the ladle sheath or coating protection in the forging process,which has the best coating effect and the oxidation loss is reduced within 3%.

KeyWords AITranslate

TaW12 alloy forging oxidation behavior protective measures

1王晖,张小明,王峰,蔡小梅.退火处理对TaW12合金力学性能及组织形貌的影响[J].稀有金属与硬质合金,2013,41(4):34-37. 被引量:5

2王晖,张小明,王峰,梁静,林小辉,蔡小梅.变形率和退火温度对TaW12合金再结晶行为的影响[J].有色金属工程,2016,6(3):13-16. 被引量:3

3吴孟海,张兴平,许德美,赵洪章,李陈.Ta-10W合金的高温断口分析[J].稀有金属,2007,31(4):434-439. 被引量:5

4张小明,王晖,张于胜,张军良.氧对钽合金热加工的影响[J].热加工工艺,2010,39(23):210-212. 被引量:8

5钱余海,李美栓,张亚明.氧化膜开裂和剥落行为[J].腐蚀科学与防护技术,2003,15(2):90-93. 被引量:22

6李韵豪.钽及钽合金塑性变形加工的感应加热(上)[J].金属加工:热加工,2016,0(19):41-44. 被引量:2

1郭雪霏,冯运莉,王宇辰.不同Al含量δ-TRIP钢铸态组织性能分析[J].华北理工大学学报:自然科学版,2019,41(2):26-30.

2彭易发,李争显,汪欣,刘林涛.ZrB_2-玻璃陶瓷复合材料的氧化行为分析[J].稀有金属材料与工程,2019,48(4):1168-1173.

3李蕾,王兴达,韩泳平.朱砂生品和炮制品X-射线衍射Fourier指纹图谱比较研究[J].西南民族大学学报:自然科学版,2018,44(6):568-575.

4陈浩,贺小毛,蒋鹏,赵昌德,郑富元.扭矩板锻造过程数值模拟及模具优化[J].模具工业,2019,45(4):5-8.

5邓伟强.催化油浆掺兑减渣生产道路沥青工艺研究[J].山东化工,2019,48(5):30-31. 被引量:1

6罗军明,李乐乐,黄俊,徐吉林.原位合成TiB_2/Fe复合材料的高温氧化行为[J].复合材料学报,2019,36(3):661-668. 被引量:1

7李习周,郭昌宏,李琦.铜引线框架氧化对集成电路分层的影响浅析[J].中国集成电路,2019,28(4):76-80. 被引量:1

8张玉存,张文文,沈久利.大型锻件自由锻造过程中外形尺寸和温度在线检测[J].锻造与冲压,2019,0(9):20-20.

9徐国战,吴鸣谦,徐文喜,丁继双,于献章,张立东,李成禄,杨轶.黑龙江省漠河市782高地铌多稀有金属矿床的地质特征及找矿标志[J].矿床地质,2019,38(2):382-400. 被引量:5

10周斌,马建成.浅谈新版ISO 12944-1、2、5、6章节的内容更新[J].现代涂料与涂装,2019,22(4):24-26.

Basic Information:

DOI:

Chinese Library Classification Number:TG319[金属学及工艺—金属压力加工]

Citation Information:

The oxide layer thickness and oxidation products during the forging process of TaW12 alloy were characterized by optical microscopy and XRD technology,and the macro-oxidation behavior were investigated.The results show that during unprotected forging,the surface of the alloy absorbs a lot of oxygen,resulting in seriously powdered surface and harden sub-surface,with the oxidation depth of about 300~400μm,and the oxidation product is Ta2O5.The oxidation of the alloy could be greatly reduced by the ladle sheath or coating protection in the forging process,which has the best coating effect and the oxidation loss is reduced within 3%.

quote

GB/T 7714-2015 [1] WANG Hui, ZHANG Xin, LI Yan-chao, et al. Study on Oxidation Behavior and Protective Measures of TaW12 Alloy during Forging Process[J]. Rare Metals and Cemented Carbides, 2019(2): 6-9.
MLA [1] WANG Hui, et al., "Study on Oxidation Behavior and Protective Measures of TaW12 Alloy during Forging Process." Rare Metals and Cemented Carbides, no. 2, 2019, pp. 6-9.
APA [1] WANG Hui, ZHANG Xin, LI Yan-chao, LIN Xiao-hui, WANG Feng, ZHANG Xiao-ming, & LI Lai-ping. (2019). Study on Oxidation Behavior and Protective Measures of TaW12 Alloy during Forging Process. Rare Metals and Cemented Carbides(2), 6-9.
IEEE [1] WANG Hui, ZHANG Xin, LI Yan-chao, LIN Xiao-hui, WANG Feng, ZHANG Xiao-ming, and LI Lai-ping, "Study on Oxidation Behavior and Protective Measures of TaW12 Alloy during Forging Process," Rare Metals and Cemented Carbides, no. 2, pp. 6-9, 2019. keywords: {TaW12 alloy;forging;oxidation behavior;protective measures}