Effect of Annealing on Microstructures and Hardness of Al1.5CrCuFeMnTi High Entropy Alloy AITranslate

School of Material Science and Engineering,Shenyang Aerospace University;School of Material Science and Engineering,Shenyang Aerospace University;School of Material Science and Engineering,Shenyang Aerospace University;School of Material Science and Engineering,Shenyang Aerospace University;School of Material Science and Engineering,Shenyang Aerospace University;School of Material Science and Engineering,Shenyang Aerospace University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

To study the effect of annealing treatment on microstructures and hardness of Al1.5CrCuFeMnTi high entropy alloy,the as-cast alloy was prepared by vacuum arc melting,and the morphology,crystal structure,composition distribution and hardness of the alloy obtained under isothermal annealing treatment at different temperatures were characterized by using methods of X-ray diffraction,scanning electron microscope and Vickers hardness tester.The results show that the as-cast Al1.5CrCuFeMnTi alloy is composed of an ordered and a disordered solid solution with a body-centered cubic structures,which forms a typical dendritic structure,and the characteristic of modulated structure is also observed in as-cast alloy.After annealing at 945℃,a Laves phase rich in Al,Cr and Mn with complex structure is formed.After annealing at 980℃,the Laves phase is transformed into FCC solid solution with Cr as matrix.Annealing treatment is conducive to the release of residual internal stress in as-cast alloys,which reduces the hardness of the alloys to about HV450.

KeyWords AITranslate

annealing treatment Al1.5CrCuFeMnTi high entropy alloy microstructures hardness

1刘源,李言祥,陈祥,陈敏.多主元高熵合金研究进展[J].材料导报,2006,20(4):4-6. 被引量:80

2崔普昌,张益铭,傅生,栾添,农智升.热处理对AlCrFeNiTi高熵合金组织和硬度的影响[J].稀有金属与硬质合金,2017,45(1):52-57. 被引量:3

3赵春凤,吴波,杨上金,周泽友,熊远鹏,陈祖华.热处理工艺对AlCoCrFeNiTi_(0.5)高熵合金的显微组织和硬度的影响[J].广西大学学报:自然科学版,2014,39(2):407-416. 被引量:7

4吴兴财,张伟强,秦力,张承华.退火处理对AlCoCrFeNi高熵合金组织结构及性能的影响[J].热加工工艺,2015,44(8):220-222. 被引量:11

5刘源,陈敏,李言祥,陈祥.Al_xCoCrCuFeNi多主元高熵合金的微观结构和力学性能[J].稀有金属材料与工程,2009,38(9):1602-1607. 被引量:62

1章奇,李忠文,于治水.光纤激光器制备FeNiMoCoCrTi高熵合金过程与研究综述[J].电子科技,2021,34(7):67-72.

2雷声,胡正强,申家升,刘亚峰,薛正伟,张翔.退火温度对FeCoCrNiTi高熵合金组织及性能的影响[J].材料热处理学报,2022,43(12):83-90.

1杨显,蒋杰,胡建军,曾敬.高熵合金涂层的研究进展[J].化学工程与装备,2018(3):214-216. 被引量:3

2羊求民,羊建高,陈丽勇,陈颢,唐彦渊.硬质合金粘结相研究进展[J].稀有金属与硬质合金,2019,47(2):82-86. 被引量:11

3叶奇鲁,杨钢,龚志华,杨沐鑫,陈清明.基于相形成判据和大数据系统的高熵合金设计(英文)[J].稀有金属材料与工程,2019,48(4):1059-1064. 被引量:1

4邵玉佳,袁兆静,王玲奇.淬火工艺对40Cr15Mo2VN高氮钢组织和硬度的影响[J].热处理,2019,34(2):31-33.

5熊建超,邹芹,李艳国,王明智,贺文全.WC基硬质合金刀具材料研究进展[J].金刚石与磨料磨具工程,2019,39(2):95-102. 被引量:5

6卢海滨,杨文超,湛永钟,汤宏群.原位合成TiBw/Ti-10MO新型低弹高强钛基复合材料[J].低碳世界,2019,9(3):288-289. 被引量:1

7金志军,邱萍,刘薇,曾永春.退火温度和退火时间对精密铂电阻温度计影响分析[J].计量与测试技术,2019,46(4):1-2. 被引量:6

8邹芹,李瑞,李艳国,王明智.超导材料的研究进展及应用[J].燕山大学学报,2019,43(2):95-107. 被引量:11

9冶金工业经济发展研究中心[J].冶金财会,2019,0(2):58-58.

10张小伟.陋室铭 爱莲说[J].快乐作文,2019,0(16):55-55.

Basic Information:

DOI:

Chinese Library Classification Number:TG139[一般工业技术—材料科学与工程];TG156.2[金属学及工艺—热处理]

Citation Information:

To study the effect of annealing treatment on microstructures and hardness of Al1.5CrCuFeMnTi high entropy alloy,the as-cast alloy was prepared by vacuum arc melting,and the morphology,crystal structure,composition distribution and hardness of the alloy obtained under isothermal annealing treatment at different temperatures were characterized by using methods of X-ray diffraction,scanning electron microscope and Vickers hardness tester.The results show that the as-cast Al1.5CrCuFeMnTi alloy is composed of an ordered and a disordered solid solution with a body-centered cubic structures,which forms a typical dendritic structure,and the characteristic of modulated structure is also observed in as-cast alloy.After annealing at 945℃,a Laves phase rich in Al,Cr and Mn with complex structure is formed.After annealing at 980℃,the Laves phase is transformed into FCC solid solution with Cr as matrix.Annealing treatment is conducive to the release of residual internal stress in as-cast alloys,which reduces the hardness of the alloys to about HV450.

quote

GB/T 7714-2015 [1] WANG Zi-yue, GUO Min, YU Xue, et al. Effect of Annealing on Microstructures and Hardness of Al1.5CrCuFeMnTi High Entropy Alloy[J]. Rare Metals and Cemented Carbides, 2019(2): 15-21.
MLA [1] WANG Zi-yue, et al., "Effect of Annealing on Microstructures and Hardness of Al1.5CrCuFeMnTi High Entropy Alloy." Rare Metals and Cemented Carbides, no. 2, 2019, pp. 15-21.
APA [1] WANG Zi-yue, GUO Min, YU Xue, JIANG Xiao-dan, NONG Zhi-sheng, & ZHU Jing-chuan. (2019). Effect of Annealing on Microstructures and Hardness of Al1.5CrCuFeMnTi High Entropy Alloy. Rare Metals and Cemented Carbides(2), 15-21.
IEEE [1] WANG Zi-yue, GUO Min, YU Xue, JIANG Xiao-dan, NONG Zhi-sheng, and ZHU Jing-chuan, "Effect of Annealing on Microstructures and Hardness of Al1.5CrCuFeMnTi High Entropy Alloy," Rare Metals and Cemented Carbides, no. 2, pp. 15-21, 2019. keywords: {annealing treatment;Al1.5CrCuFeMnTi high entropy alloy;microstructures;hardness}