Effect of Deformation and Annealing Temperature on the Microstructure of Tantalum Plate AITranslate
Abstract AITranslate
The surface and microstructure of the deep-drawn tantalum shell is observed by scanning electron microscope and optical microscope and effect of deformation and annealing treatment on the microstructure of tantalum plates is studied. It shows that grain refinement is very important to assure good surface quality of deep-drawn Ta shell. More cold-rolled deformation prior to annealing is good for finer grain for pure Ta produced by electron-beam smelting,with 90% rolling deformation, initial recrystallization temperature about 800 ℃ ,finer grain can be obtained after annealing at 850 ℃ for 40 min. And proper high-temperature short-time annealing can make grain finer.
KeyWords AITranslate
1刘世友.钽在高新技术中的应用[J].稀有金属与硬质合金,1998,26(2):55-57. 被引量:28
2沙穆素诺夫ГВ 卜宝林 译.钽与铌[M].北京:中国工业出版社,1962..
3彭宝霞.关于使用固钽和液体钽电容的浅释[J].电子产品可靠性与环境试验,1999,0(4):22-25. 被引量:7
4PrabhatKumar,HenningUhlenhut,李学芳,佘建芳.粉末冶金钽制品的最新进展[J].国外难熔金属与硬质材料,2003,19(2):57-63. 被引量:2
5Gottstein G.Rekristallisation Metallischer Werkstoffe[M].Leipzing:VEB Deutscher Verlag Fur Grundstoffirdust,1966.79.
1周伟,陈军,赵永庆,曲恒磊,冯亮,郭荻子.钽钛合金再结晶退火工艺研究[J].热加工工艺,2006,35(20):61-63. 被引量:4
2周伟,陈军,赵永庆,曲恒磊,冯亮,郭荻子.钽钛合金的再结晶动力学研究[J].稀有金属材料与工程,2007,36(10):1824-1826. 被引量:1
3张炎,王再友,查光成.热处理对钽板组织和力学性能的影响[J].热加工工艺,2011,40(24):218-221. 被引量:2
4潘文高,陈炜晔,吴澜尔.钽材轧制和再结晶织构演变研究进展[J].材料导报,2016,30(21):150-156.
5李娜.钽壳表面的结瘤和预防措施[J].中国金属通报,2018(11):69-70.
6杨光,马贤,王丁丁,卢肖勇,吕绪明,罗立平.高温金属蒸气环境对难熔金属钽的影响[J].科技视界,2020(28):14-16.
7张倩,李秀青,魏世忠,王琪,张程,徐流杰,周玉成.冷变形及退火对Ta-2.5W合金微观组织及力学性能的影响[J].稀有金属与硬质合金,2022,50(2):50-56.
1温军国,郑弃非,赵云豪,涂思京,李德富.冷变形及热处理工艺对0Cr17Ni钢组织和性能的影响[J].热加工工艺,2007,36(12):55-57. 被引量:1
2张奕,郑永键,唐晓东,付宝全,王虎,雷锦文.变形率和热处理制度对Nb47Ti合金显微组织的影响[J].中国有色金属学报,2010,20(B10):331-335. 被引量:4
3季良,杨武雄,肖荣诗.金属钽箔十字交叉激光微点焊工艺研究[J].应用激光,2013,33(6):601-605. 被引量:2
4曾祥勇,李龙,周德敬.4A60铝/08Al钢复合带材冷轧复合后钢的再结晶行为[J].材料热处理学报,2015,36(8):73-78.
5马凡蛟,王毓,赖运金,侯峰起,李少强,雷锦文,杜予晅,张平祥.Ti45Nb钛合金再结晶行为研究[J].热加工工艺,2017,46(12):232-234. 被引量:2
6张亚峰,于振涛,余森,贺新杰,汶斌斌,刘汉源,何卫敏,赵利渊.TA16钛合金管材拉伸性能及组织研究[J].广州化工,2018,46(9):30-32. 被引量:1
7刘新利,宋晓毓,王德志.铌/钢和钽/钛/钢层状复合材料中铌层和钽层的氢化剥离回收[J].稀有金属与硬质合金,2022,50(6):59-67.
1黄静娴.冶炼工艺对18—8不锈钢力学性能的影响[J].沪昌科技,1996(6):32-34.
2郭瑞鹏,崔岩,贵永亮.冷变形量对低碳冷轧板组织及再结晶温度的影响[J].钢铁钒钛,2014,35(4):122-126. 被引量:6
3杨振东.提高球团入炉生球质量的生产实践[J].北方钒钛,2014,0(4):4-6.
4孟德田,杨树明,隋孝利.承钢竖炉球团配加钠基膨润土的研究与应用[J].四川冶金,2005,27(5):10-12. 被引量:1
5严丽.提高纯铝电子负极箔材比电容的工艺研究[J].黑龙江冶金,1995,0(3):20-22.
6阎秀清,王劲松,王继伟.30tEBT-40tLF冶炼工艺浅析[J].鞍钢技术,1999(5):44-48. 被引量:1
7刘建涛,刘国权,胡本芙,宋月鹏,张义文,陶宇.FGH96合金静态再结晶行为的研究[J].材料热处理学报,2005,26(6):12-15. 被引量:5
8张立,陈述,SchubertWD,黄伯云.Ce在混合稀土掺杂的硬质合金烧结体表面富集现象的热力学分析[J].硬质合金,2004,21(2):70-76. 被引量:8
9直接退火——一种新的430铁素体不锈钢生产线[J].特钢技术,2006,11(2):6-6.
10王梅英.影响煅烧用石灰石质量的几个因素[J].河南冶金,1997(A09):69-70. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF146.416[冶金工程—冶金物理化学]
Citation Information:
The surface and microstructure of the deep-drawn tantalum shell is observed by scanning electron microscope and optical microscope and effect of deformation and annealing treatment on the microstructure of tantalum plates is studied. It shows that grain refinement is very important to assure good surface quality of deep-drawn Ta shell. More cold-rolled deformation prior to annealing is good for finer grain for pure Ta produced by electron-beam smelting,with 90% rolling deformation, initial recrystallization temperature about 800 ℃ ,finer grain can be obtained after annealing at 850 ℃ for 40 min. And proper high-temperature short-time annealing can make grain finer.
quote
| GB/T 7714-2015 | [1] ZHANG Xing-jian, WANG Zhi-fa, CHEN De-xin, et al. Effect of Deformation and Annealing Temperature on the Microstructure of Tantalum Plate[J]. Rare Metals and Cemented Carbides, 2005(4): 8-12. |
| MLA | [1] ZHANG Xing-jian, et al., "Effect of Deformation and Annealing Temperature on the Microstructure of Tantalum Plate." Rare Metals and Cemented Carbides, no. 4, 2005, pp. 8-12. |
| APA | [1] ZHANG Xing-jian, WANG Zhi-fa, CHEN De-xin, & ZHANG Jin-jin. (2005). Effect of Deformation and Annealing Temperature on the Microstructure of Tantalum Plate. Rare Metals and Cemented Carbides(4), 8-12. |
| IEEE | [1] ZHANG Xing-jian, WANG Zhi-fa, CHEN De-xin, and ZHANG Jin-jin, "Effect of Deformation and Annealing Temperature on the Microstructure of Tantalum Plate," Rare Metals and Cemented Carbides, no. 4, pp. 8-12, 2005. keywords: {tantalum;deformation rate;annealing temperature;recrystallization;eletron beam melting} |