Study on Application of WC/Steel Composite Material for Guide Rollers AITranslate

School of Materials Science and Engineering, Anhui University of Technology;School of Materials Science and Engineering, Anhui University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Based on the contrast tests between the WC/steel composite material ( code GJH-2 alloy) and the Gx cast alloy used in bar or wire mill for guide rollers, discussion is made on the future application of the WC/steel composite material in the hot-worked die. The contrast test results showed that GJH- 2cermet is characterized by good high-temperature wear resistance under corresponding heat treatment at 450-650℃ with heavy load and sliding velocity above 2 m/s.

KeyWords AITranslate

WC/steel composite material high-temperature wear guide rollers application

1李沐山.国外钢结硬质合金新进展[J].硬质合金,1994,11(2):105-114. 被引量:50

2王荣滨,红梅.热冲压用DT钢结硬质合金角冲头复合强化处理研究[J].硬质合金,1995,12(4):233-237. 被引量:3

3H,BK,李沐山.凿岩工具用碳化物钢基耐磨材料的研制[J].国外难熔金属与硬质材料,1994,10(2):28-29. 被引量:2

4肖玉麟.美国钢结硬质合金的若干应用实例[J].硬质合金,1986,5(2):47-47.

5刘光俊.金属加工用的硬质合金轧辊进展[J].硬质合金,1994,11(1):44-52. 被引量:6

6高彩桥.金属的摩擦磨损与热处理[M].北京:机械工业出版社,1988..

1王晓灵.TiC硬质合金导辊的失效原因分析[J].轧钢,2012,29(2):67-70.

1陈其伟.高温磨损试验参数对WC/钢复合材料高温磨损特性的影响[J].稀有金属与硬质合金,2005,33(1):22-25. 被引量:1

2马建国,叶劲,尤显卿,刘宝.离心铸造WC/钢复合材料显微组织[J].材料热处理学报,2009,30(6):130-134. 被引量:1

3陈其伟.热处理对WC/钢复合材料高温磨损特性的影响[J].稀有金属与硬质合金,2004,32(4):10-13. 被引量:1

4尤显卿.热处理条件对WC/钢复合材料热疲劳性能的影响[J].兵器材料科学与工程,2004,27(6):23-26. 被引量:3

5陈其伟.提高轧机导卫辊寿命的研究[J].钢铁研究学报,2002,14(3):25-29. 被引量:2

6黄曼平,尤显卿,张成军,马建国.电冶熔铸WC/钢复合材料表面激光重熔工艺[J].金属热处理,2008,33(9):19-24. 被引量:1

7尤显卿,马建国,宋雪峰,任昊,黄曼平.电冶熔铸WC/钢复合材料中WC的溶解行为[J].中国有色金属学报,2005,15(9):1363-1368. 被引量:17

8尤显卿.GJW35钢结硬质合金热疲劳裂纹萌生初步探讨[J].硬质合金,1999,16(2):71-74. 被引量:6

9尤显卿,任昊,郑玉春,斯廷智.电渣熔铸WC/钢复合材料的磨损性能研究[J].特种铸造及有色合金,2003(6):19-21. 被引量:9

10尤显卿,王基才,郑玉春,黄漫平,袁根福.铸造WC/钢复合材料的锻造研究[J].热加工工艺,2002,31(6):40-42. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TG146.4[金属学及工艺—金属材料]

Citation Information:

Based on the contrast tests between the WC/steel composite material ( code GJH-2 alloy) and the Gx cast alloy used in bar or wire mill for guide rollers, discussion is made on the future application of the WC/steel composite material in the hot-worked die. The contrast test results showed that GJH- 2cermet is characterized by good high-temperature wear resistance under corresponding heat treatment at 450-650℃ with heavy load and sliding velocity above 2 m/s.

quote

GB/T 7714-2015 [1] REN Xiang, CHEN Qi-wei. Study on Application of WC/Steel Composite Material for Guide Rollers[J]. Rare Metals and Cemented Carbides, 2005(4): 4-7.
MLA [1] REN Xiang, and CHEN Qi-wei. "Study on Application of WC/Steel Composite Material for Guide Rollers." Rare Metals and Cemented Carbides, no. 4, 2005, pp. 4-7.
APA [1] REN Xiang, & CHEN Qi-wei. (2005). Study on Application of WC/Steel Composite Material for Guide Rollers. Rare Metals and Cemented Carbides(4), 4-7.
IEEE [1] REN Xiang and CHEN Qi-wei, "Study on Application of WC/Steel Composite Material for Guide Rollers," Rare Metals and Cemented Carbides, no. 4, pp. 4-7, 2005. keywords: {WC/steel composite material;high-temperature wear;guide rollers;application}