Study of WC Ceramic Tool Material by SiC Whisker Toughening AITranslate
Abstract AITranslate
The composition and hot-pressing parameters of WC/SiCw ceramic composite were optimized through orthogonal experiment. Compared with those of the pure WC, the bending strengh, fracture toughness and Vicker's hardness of the optimized WC/SiCw composite are increased by 50%, 30% -40%, and 10% - 15 % respectively. The cutting test results show that the optimized WC/SiCw composite ceramic cutting tool material exhibit superior turning properties to similar hard alloy material, indicating that it is feasible to toughen the WC ceramic cutting tool material by using SiCw instead of metallic binding phase.
KeyWords AITranslate
1季光.晶须增韧陶瓷刀具评述[J].工具技术,1994,28(4):39-40. 被引量:5
2Becher P F.Microstructural design of toughened ceramics[J],J Am Ceram Soc,1991,74:225.
3Xia K,et al.Examination on fracture surfaces of SiC-whisker-reinforced alumina after high-temperature creep deformation[J],J Mater Sci,1994,29:5219.
1李喜宝,柯昌明,李楠.SiC晶须增韧陶瓷基复合材料的研究进展[J].材料导报,2007,21(F05):394-397. 被引量:10
2刘永姜,王爱玲,朱丽梅,王彪.SiC晶须增韧光敏树脂的力学性能影响因素研究[J].兵器材料科学与工程,2009,32(6):66-70. 被引量:3
3王秋红,郑勇,孙帆,高小龙.碳化硅晶须的制备及其在复合材料增韧中的应用[J].硬质合金,2010,27(1):49-54. 被引量:10
4彭进,郝德辉,邹文俊,董企铭,朱俊芳.氮化硅晶须表面化学镀镍及应用研究[J].表面技术,2011,40(3):36-39. 被引量:2
5Jialin Sun,Jun Zhao,Zhifu Huang,Ke Yan,Xuehui Shen,Jiandong Xing,Yimin Gao,Yongxin Jian,Hejie Yang,Bo Li.A Review on Binderless Tungsten Carbide: Development and Application[J].纳微快报:英文版,2020,12(1):158-194. 被引量:7
1耿海涛,阎峰云,狄正贤,李静娟.氟化铝对红柱石莫来石化的影响[J].硅酸盐通报,2012,31(2):345-348. 被引量:4
2冯立超,乔斌,贺毅强,于雪梅.深海装备材料之陶瓷基复合材料的研究进展[J].热加工工艺,2012,41(22):132-136. 被引量:4
3李海艳,侯清麟,银锐明,谭凯铭,计富宝,李蓉.添MgO-Y_2O_3的Fe-Mo包覆Si_3N_4复合粉末反应烧结中组织形成与演化分析[J].硬质合金,2013,30(2):66-72. 被引量:1
4计富宝,银锐明,李海艳,周晓波,谭凯铭.烧结温度对多机制耦合增韧Si_3N_4陶瓷微观组织及力学性能的影响[J].硬质合金,2013,30(3):122-128.
5计富宝,银锐明,陈丹,李海艳,周晓波,谭凯铭.金属Mo元素对双金属增韧Si_3N_4陶瓷组织与力学性能影响[J].硬质合金,2013,30(4):181-189. 被引量:2
6刘龙阳,陈险峙,余辉,陈拥军,骆丽杰,李崴,李建保.SiCw/SiCp质量比对Al2O3/ZrO2/SiC复合陶瓷力学性能的影响[J].陶瓷学报,2018,39(6):728-734.
7梁欣,陈常连,周诗聪,季家友,朱丽,黄志良,徐慢.碳化硅添加对氮化硅转化为碳化硅晶粒形貌的影响[J].武汉工程大学学报,2019,41(1):60-64. 被引量:2
8陈永杰,徐三魁,王海阔,彭进,邹文俊,邵华丽.高韧性聚晶立方氮化硼(PcBN)复合片的研究进展[J].山东化工,2015,44(2):43-45.
9成来飞,解玉鹏,梅辉,张立同.化学气相渗透制备SiC_w/SiC层状结构陶瓷[J].科学通报,2015,60(3):300-308. 被引量:1
10伍璧超,卢玉斌.三维激光成型固化光敏树脂的力学性能研究[J].西南科技大学学报,2015,30(3):21-24. 被引量:4
1曹玉军,刘杰.SiC晶须增韧WC陶瓷刀具材料的研究[J].硬质合金,2005,22(3):161-166. 被引量:4
2北京工业大学成功开发A1203陶瓷刀片[J].模具工程,2004(4):13-13.
3萧虹,艾兴.晶须增韧陶瓷刀具材料的磨损机理[J].机械工程学报,1992,28(3):1-5. 被引量:2
4李建保,黄勇.新型陶瓷刀具材料的研究与开发[J].现代技术陶瓷,1993(1):7-13. 被引量:2
5季光.晶须增韧陶瓷刀具[J].机械工人:冷加工,1994(1):10-11.
6韩韡,许晓静,刘延山.硬质合金刀具材料的研究现状与发展思路[J].工具技术,2002,36(10):3-8. 被引量:15
7刘记伟,罗建华,刚建伟.2219铝合金Φ42mm×15mm管材的生产工艺研究[J].轻合金加工技术,2012,40(7):51-53. 被引量:1
8邓建新,艾兴.陶瓷刀具材料的增韧补强研究[J].工具技术,1995,29(1):36-38. 被引量:3
9黄守伟.浅谈硬质合金刀具[J].经济技术协作信息,2012(13):94-94.
10潘敏元,赵高扬,陈宇航,文保平,潘明.高强韧性复合陶瓷刀具材料的研究[J].陕西机械学院学报,1992,8(3):161-172.
Basic Information:
DOI:
Chinese Library Classification Number:TG148[金属学及工艺—金属材料]
Citation Information:
The composition and hot-pressing parameters of WC/SiCw ceramic composite were optimized through orthogonal experiment. Compared with those of the pure WC, the bending strengh, fracture toughness and Vicker's hardness of the optimized WC/SiCw composite are increased by 50%, 30% -40%, and 10% - 15 % respectively. The cutting test results show that the optimized WC/SiCw composite ceramic cutting tool material exhibit superior turning properties to similar hard alloy material, indicating that it is feasible to toughen the WC ceramic cutting tool material by using SiCw instead of metallic binding phase.
quote
| GB/T 7714-2015 | [1] CAO Yu-jun, LIU Jie. Study of WC Ceramic Tool Material by SiC Whisker Toughening[J]. Rare Metals and Cemented Carbides, 2005(4): 13-16. |
| MLA | [1] CAO Yu-jun, and LIU Jie. "Study of WC Ceramic Tool Material by SiC Whisker Toughening." Rare Metals and Cemented Carbides, no. 4, 2005, pp. 13-16. |
| APA | [1] CAO Yu-jun, & LIU Jie. (2005). Study of WC Ceramic Tool Material by SiC Whisker Toughening. Rare Metals and Cemented Carbides(4), 13-16. |
| IEEE | [1] CAO Yu-jun and LIU Jie, "Study of WC Ceramic Tool Material by SiC Whisker Toughening," Rare Metals and Cemented Carbides, no. 4, pp. 13-16, 2005. keywords: {ceramic composite;whisker;hot- pressing toughening;WC/SiCw} |