Research of lowPressure HIP for RegeneratingMining Cemented Carbide AITranslate
Abstract AITranslate
The mining cemented carbide was regenerated by lowpressure HIP. The results show the increase in the fransverse rupture strength and the decrease in the porosity(to A00). The service life of the regenerated cemented carbide is similar to that of conventional cemented carbide. The mechanism of the denisfication of lowpressure HIP is analysed.
KeyWords AITranslate
1张俊熙,王和斌.用电溶法回收的碳化钨制取的矿用硬质合金的特性及其使用效果[J].硬质合金,1993,10(3):133-142. 被引量:1
2孙宝琦.关于我国废残硬质合金回收与再生问题的一些看法.硬质合金质量分析论文(内部资料)[M].,1997,8..
3黄健民.第六次全国硬质合金学术会议论文集[M].,1995.151.
1张兴华,汪明朴.再生碳化钨性能及应用[J].硬质合金,2008,25(1):58-62. 被引量:7
1廖军,吴翔,江庆.烧结温度对含再生料硬质合金性能的影响[J].四川有色金属,2013(2):45-48. 被引量:3
2魏仕勇,付青峰,万珍珍,陈志宝.再生WC-Co粉与混合稀土制备YG8硬质合金存在的脱碳问题研究[J].江西科学,2014,32(4):439-442. 被引量:1
3魏仕勇,万珍珍,付青峰,尹桦.再生WC-Co粉制备硬质合金的研究[J].热处理技术与装备,2014,35(5):18-21.
4林中坤,林晨光,曹瑞军.国内外硬质合金再生利用的现状与对策[J].硬质合金,2014,31(5):315-321. 被引量:19
5魏仕勇,万珍珍,付青峰,陈志宝.混合稀土氧化物与再生WC-Co粉制备YG8硬质合金的研究[J].热加工工艺,2015,44(14):55-58. 被引量:3
6史顺亮,吴翔,江庆.不同再生原料添加比例对WC-10%Co硬质合金性能的影响[J].四川冶金,2015,37(4):14-17. 被引量:1
7周新华,王力民,彭英健.我国硬质合金再生产业现状与发展[J].硬质合金,2016,33(5):356-364. 被引量:19
1王跃明,熊翔,解路,徐玄,闵小兵.钨异形件等离子喷涂近净成形技术研究[J].中南大学学报:自然科学版,2012,43(4):1267-1275. 被引量:7
2刘荣湘,易凯华.镍代钴矿用硬质合金的新进展[J].稀有金属与硬质合金,1994,22(2):46-49. 被引量:6
3印红羽,盛挺,汪海宽.硬质合金低压热等静压烧结工艺[J].粉末冶金技术,1997,15(4):299-303. 被引量:16
4张俊熙,王和斌.用电溶法回收的碳化钨制取的矿用硬质合金的特性及其使用效果[J].硬质合金,1993,10(3):133-142. 被引量:1
5王国栋,商鸿亮.颗粒增强复合材料研究及矿用硬质合金进展[J].山东化工,2015,44(6):68-70. 被引量:2
6自贡硬质合金厂Z系列矿用硬质合金获总公司技术进步四等奖[J].中国钨业,1993,0(6):17-17.
7文道维,宋秀凤,高秀玲.1Cr17Ni2马氏体不锈钢的力学性能及抗腐蚀性能的研究[J].大电机技术,1997(2):33-38. 被引量:14
8吴冲浒,聂洪波,肖满斗,谢海唯.纳米材料在硬质合金中的应用[J].中国材料进展,2014,33(1):39-45. 被引量:7
9黄建民,吕海波.微细晶粒WC-Co硬质合金低压热等静压处理[J].硬质合金,1996,13(3):142-145. 被引量:9
10长春数控研发成功国内首台125t全自动摩擦焊机[J].制造技术与机床,2007(2):5-5.
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程];TF124.32[冶金工程—粉末冶金]
Citation Information:
The mining cemented carbide was regenerated by lowpressure HIP. The results show the increase in the fransverse rupture strength and the decrease in the porosity(to A00). The service life of the regenerated cemented carbide is similar to that of conventional cemented carbide. The mechanism of the denisfication of lowpressure HIP is analysed.
quote
| GB/T 7714-2015 | [1] ZHOU Jian-hua, SUN Bao-qi. Research of lowPressure HIP for RegeneratingMining Cemented Carbide[J]. Rare Metals and Cemented Carbides, 1999(2): 19-21. |
| MLA | [1] ZHOU Jian-hua, and SUN Bao-qi. "Research of lowPressure HIP for RegeneratingMining Cemented Carbide." Rare Metals and Cemented Carbides, no. 2, 1999, pp. 19-21. |
| APA | [1] ZHOU Jian-hua, & SUN Bao-qi. (1999). Research of lowPressure HIP for RegeneratingMining Cemented Carbide. Rare Metals and Cemented Carbides(2), 19-21. |
| IEEE | [1] ZHOU Jian-hua and SUN Bao-qi, "Research of lowPressure HIP for RegeneratingMining Cemented Carbide," Rare Metals and Cemented Carbides, no. 2, pp. 19-21, 1999. keywords: {lowpressure HIP;regenerated;mining cemented carbide;densification} |