daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

An Investigation of Magnetostriction Propertyaffected by Mn Content for Triple System Alloy RxR1-xFe AITranslate

Department of Materials Department of Zhongnan University of Technology;Department of Materials Department of Zhongnan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The TbDyFeMn system alloys are prepared by arc melting in an inert atmosphere water cooled copper hearth and by float zone melting (ZM) technique. By measuring the ascast rod sample's magnetostriction and analyzing its microstructures with EPMA and Laue Xray techniques, it is found that the content of element Mn affects both the material's magnetostriction properties and the microstructure. The optimum content of element Mn in this material for maximum magnetostriction is given. It offers the convincing foundation for the development of the giant magnetostriction materials.

KeyWords AITranslate

RFe system alloys giant magnetostriction float zone melting microscopic analysis

1Verhoevon J D 卞纪(译).-[J].国外金属材料,1991,(3):19-19.

2蒋志红.-[J].稀土,1991,12(1):19-19.

1黎文献,余琨,谭敦强,马正青,陈鼎.稀土超磁致伸缩材料的研究[J].矿冶工程,2000,20(3):64-67. 被引量:13

1孙乐,刘信恩,郑晓静.薄膜—基体型磁致伸缩微致动器的数值模拟[J].应用力学学报,2004,21(2):41-45. 被引量:5

2李恒菊,李银祥,邓志刚,姚向东,张立军.磁致伸缩微位移工作台的新型定位方法[J].磁性材料及器件,2005,36(1):29-31. 被引量:3

3李寅博,曾海泉.超磁致伸缩功率超声换能器振动系统分析[J].机械工程与自动化,2010(4):13-15.

4李玉山,刘海斌,赵浩达,庞海昭,韩志群,龚晓钟.AAO模板法制备的稀土TbFe合金纳米线及其磁学性能[J].磁性材料及器件,2013,44(4):19-23. 被引量:1

5程建建,祝志芳,周强,陈豪,李春龙.基于稀土TbDyFe合金的新型流量阀的设计[J].科技广场,2014(2):247-249.

6王传礼,方平,丁凡.GMM在机械电子工程中的应用研究现状[J].电子机械工程,2002,18(4):1-4. 被引量:6

7王传礼,丁凡,张凯军.超磁致伸缩执行器及其在微小流体泵中的应用[J].液压与气动,2002,26(11):26-28. 被引量:3

8杨帆,徐明舟.超磁致伸缩材料研究及应用现状[J].金属材料研究,2021,47(1):18-21.

9Chengde Gao,Zihao Zeng,Shuping Peng,Cijun Shuai.Magnetostrictive alloys:Promising materials for biomedical applications[J].生物活性材料(英文),2022,7(2):177-195.

10王传礼,丁凡.基于新型功能材料的高频响电液伺服阀[J].矿冶工程,2002,22(4):79-81. 被引量:2

1刘国征,丁开鸿,李泽军,闫建明,谢宏祖.氮化Sm_2Fe_(17)合金的结构与磁性能[J].稀土,1994,15(5):8-10.

2张其文,宋晓艳,刘雪梅,王海滨,张忠健.梯度超粗晶硬质合金的制备与组织性能研究[J].硬质合金,2016,33(1):8-13. 被引量:3

3朱镭,吴庆平.氧化镁值的意义及影响因素[J].铸造,1992(9):38-40. 被引量:2

4王仁芳,崔志武.稀土铁合金及其化合物中稀土总量与铁量的联合测定方法研究[J].江西有色金属,1998,12(3):44-48. 被引量:4

5朱厚卿.稀土超磁致伸缩材料的应用[J].应用声学,1998,17(5):3-10. 被引量:32

6胡轶嵩,金浩,刘荣华,崔玉友,线全刚,杨锐.光学浮区法制备定向生长Ti-44.5Al-3Nb-0.8Si-0.2C合金[J].材料热处理学报,2014,35(9):45-48. 被引量:1

7高培虎,张延京,王强,杨忠,郭永春,李建平.灰铸铁内部石墨定向生长研究[J].热加工工艺,2016,45(11):86-89. 被引量:2

8石洁,罗超,王怀胜,刘勇,李鱼飞.感应区域熔炼法制备高纯铜[J].稀有金属材料与工程,2010,39(A01):418-421. 被引量:6

9政策[J].中国有色金属,2011(12):19-20.

10丁贤飞,林均品,张来启,王艳丽,叶丰,陈国良.高Nb-TiAl合金定向凝固组织的研究[J].材料工程,2009,37(S1):258-262. 被引量:8

Basic Information:

DOI:

Chinese Library Classification Number:TG132.27[一般工业技术—材料科学与工程]

Citation Information:

The TbDyFeMn system alloys are prepared by arc melting in an inert atmosphere water cooled copper hearth and by float zone melting (ZM) technique. By measuring the ascast rod sample's magnetostriction and analyzing its microstructures with EPMA and Laue Xray techniques, it is found that the content of element Mn affects both the material's magnetostriction properties and the microstructure. The optimum content of element Mn in this material for maximum magnetostriction is given. It offers the convincing foundation for the development of the giant magnetostriction materials.

quote

GB/T 7714-2015 [1] WEN Xian-zhe, YU Wei-qiang. An Investigation of Magnetostriction Propertyaffected by Mn Content for Triple System Alloy RxR1-xFe[J]. Rare Metals and Cemented Carbides, 1999(2): 11-14.
MLA [1] WEN Xian-zhe, and YU Wei-qiang. "An Investigation of Magnetostriction Propertyaffected by Mn Content for Triple System Alloy RxR1-xFe." Rare Metals and Cemented Carbides, no. 2, 1999, pp. 11-14.
APA [1] WEN Xian-zhe, & YU Wei-qiang. (1999). An Investigation of Magnetostriction Propertyaffected by Mn Content for Triple System Alloy RxR1-xFe. Rare Metals and Cemented Carbides(2), 11-14.
IEEE [1] WEN Xian-zhe and YU Wei-qiang, "An Investigation of Magnetostriction Propertyaffected by Mn Content for Triple System Alloy RxR1-xFe," Rare Metals and Cemented Carbides, no. 2, pp. 11-14, 1999. keywords: {RFe system alloys;giant magnetostriction;float zone melting;microscopic analysis}