Influence of the Microstructure on the ThermalFatigue Properties of Steel Bonded Carbide GJW35 AITranslate

Hefei University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Z]The microstructure of steel bonded carbide GJW35 after heat treatment has been analysed, and influence of the microstructure on the nucleation and propagation of thermal fatigue cracks of this alloy has been studied. The results show that the thermal fatigue cracks nucleate and propagate preferentially in the hard phase, and the nucleation and propagation are stoped by the steel based phase. By improving microstructure, the thermal fatigue resistance of this alloy can be raised.

KeyWords AITranslate

steel bonded carbide microstructure thermal fatigue.

1李健 束德林 等.-[J].安徽工学院学报,1985,(3):12-12.

2尤显卿.-[J].硬质合金,1995,(1):61-61.

1司乃潮,郭毅,李国强.稀土Ce对Al-Cu4.5%合金热疲劳性能的影响[J].中国有色金属学报,2006,16(4):606-611. 被引量:19

2司乃潮,吴强,李国强.Ti对Al-4.5%Cu合金热疲劳性能的影响[J].铸造,2006,55(7):731-734. 被引量:9

1罗天骄,姚广春,吴林丽,刘宜汉,韩变华.CeO_2在镀镍碳纤维增强铝合金基复合材料中的作用[J].中国有色金属学报,2007,17(1):80-84. 被引量:5

2肖代红,陈康华,宋旼.铈对Al-Cu-Mg-Mn-Ag合金时效析出与显微组织的影响[J].中国有色金属学报,2007,17(5):669-675. 被引量:19

3郭洪飞,郝新,何智慧,高文海.稀土La对45Cr2NiMoVSi热作模具钢力学性能的影响[J].铸造技术,2007,28(8):1079-1083. 被引量:10

4高文海,郭洪飞,郝新,何智慧.镧对5CrMnMo热作模具钢力学性能的影响[J].稀有金属,2007,31(4):467-471. 被引量:4

5李慧中,梁霄鹏,李芳芳,郭菲菲,李洲,张新明.Effect of Y content on microstructure and mechanical properties of 2519 aluminum alloy[J].中国有色金属学会会刊:英文版,2007,17(6):1194-1198. 被引量:6

6贾淑果,刘平,郑茂盛,任凤章,田保红,周根树.铜合金固溶强化的电子理论解释[J].中国有色金属学报,2008,18(8):1522-1526. 被引量:14

7张国栋,苏彬,何玉怀,黄朝晖,赵希宏.IC10合金热机械疲劳性能与寿命预测[J].中国有色金属学报,2009,19(1):62-69. 被引量:2

8司乃潮,华雄飞,司松海,袁婷婷,李达云.La对定向凝固Al-4.5%Cu合金热疲劳性能的影响[J].铸造,2009,58(3):262-265. 被引量:3

9郝新,郭洪飞,高文海,刘景顺,何智慧.Effects of Lanthanum on Mechanical Properties of 5CrNiMo Forging Die Steel[J].稀土学报:英文版,2007,0(S2):254-257.

10应建中,谢世坤,易荣喜,张庭芳.稀土Ce对Al4.5Cu合金性能的影响[J].热加工工艺,2009,38(22):11-13. 被引量:1

1徐建刚,游兴河,王成福.粉末冶金材料抗热疲劳性能的研究现状[J].粉末冶金技术,1990,8(3):179-183.

2刘传博,韩洪浩.4Cr5MoSiV1(H13)电渣钢热疲劳性能的试验研究[J].特殊钢,1995,16(3):16-18. 被引量:3

3赵晗,翁韶华,陈栋,周小明.连铸方坯低倍边部裂纹原因分析[J].物理测试,2004,22(4):30-33. 被引量:2

4舒鸫鹏.复合添加碳化钒石墨烯对数控机床刀具钢性能的影响[J].钢铁钒钛,2016,37(5):50-53. 被引量:1

5季业益,陆宝山,孙书娟,李强伟.V-Ti增强相含量对表面改性模具性能的影响[J].钢铁钒钛,2016,37(5):65-69. 被引量:1

6刘宝,尤显卿,陈丽娜,张炎.离心铸造LGJW20钢结硬质合金热疲性能研究[J].硬质合金,2009,26(3):165-171.

7尤显卿,郑玉春,程娟文,任昊.热应力作用下碳化钨基钢结硬质合金梯形裂纹的形成机理[J].中国有色金属学报,2003,13(5):1098-1102. 被引量:6

8尤显卿.GJW35钢结硬质合金热疲劳裂纹萌生初步探讨[J].硬质合金,1999,16(2):71-74. 被引量:6

9张焱,丁峰,尤显卿,叶劲,刘宝.钢结硬质合金GJW50热疲劳开裂的探讨[J].硬质合金,2008,25(4):227-231. 被引量:3

10尤显卿.GJW35钢结硬质合金热疲劳裂纹扩展的观察[J].硬质合金,2000,17(2):92-95. 被引量:9

Basic Information:

DOI:

Chinese Library Classification Number:TF125.32[冶金工程—粉末冶金]

Citation Information:

Z]The microstructure of steel bonded carbide GJW35 after heat treatment has been analysed, and influence of the microstructure on the nucleation and propagation of thermal fatigue cracks of this alloy has been studied. The results show that the thermal fatigue cracks nucleate and propagate preferentially in the hard phase, and the nucleation and propagation are stoped by the steel based phase. By improving microstructure, the thermal fatigue resistance of this alloy can be raised.

quote

GB/T 7714-2015 [1] YOU Xian-qing. Influence of the Microstructure on the ThermalFatigue Properties of Steel Bonded Carbide GJW35[J]. Rare Metals and Cemented Carbides, 1999(2): 22-27.
MLA [1] YOU Xian-qing. "Influence of the Microstructure on the ThermalFatigue Properties of Steel Bonded Carbide GJW35." Rare Metals and Cemented Carbides, no. 2, 1999, pp. 22-27.
APA [1] YOU Xian-qing. (1999). Influence of the Microstructure on the ThermalFatigue Properties of Steel Bonded Carbide GJW35. Rare Metals and Cemented Carbides(2), 22-27.
IEEE [1] YOU Xian-qing, "Influence of the Microstructure on the ThermalFatigue Properties of Steel Bonded Carbide GJW35," Rare Metals and Cemented Carbides, no. 2, pp. 22-27, 1999. keywords: {steel bonded carbide, microstructure, thermal fatigue.}