Highly Selective Oxidation of Styrene to Styrene Oxide over a Tetraphenylporphyrin-Bridged Silsesquioxane-Based Hybrid Porous Polymer AITranslate

Shandong University; Shandong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Two silsesquioxane-based hybrid porous polymers (PcsM and PcsH) were easily synthesized by the Friedel–Crafts reaction of tetraphenylporphyrin derivative (HTPP and MnTPP) with octavinylsilsesquioxane (OVS) applying AlCl3 as catalyst. A series of characterization results demonstrate that the materials have been successfully prepared. PcsM and PcsH act as effective catalysts to selectively oxidize styrene to styrene oxide with oxygen as a green and economical oxidant. The effects of reaction conditions on the reaction activity, such as reaction energy, reaction time, solvent type, catalyst dosage, etc., were systematically discussed. Under optimized conditions, the conversion rate of styrene was 99.9%, and the yield of styrene oxide could reach 80.6%. Moreover, the reaction mechanism of selective oxidation of styrene to styrene oxide using PcsM as a catalyst is reasonably proposed. Importantly, PcsM shows an excellent recyclable performance.

KeyWords AITranslate

silsesquioxane porous polymer styrene oxidation heterogeneous catalysis porphyrin
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00547

Chinese Library Classification Number:

Citation Information:

Two silsesquioxane-based hybrid porous polymers (PcsM and PcsH) were easily synthesized by the Friedel–Crafts reaction of tetraphenylporphyrin derivative (HTPP and MnTPP) with octavinylsilsesquioxane (OVS) applying AlCl3 as catalyst. A series of characterization results demonstrate that the materials have been successfully prepared. PcsM and PcsH act as effective catalysts to selectively oxidize styrene to styrene oxide with oxygen as a green and economical oxidant. The effects of reaction conditions on the reaction activity, such as reaction energy, reaction time, solvent type, catalyst dosage, etc., were systematically discussed. Under optimized conditions, the conversion rate of styrene was 99.9%, and the yield of styrene oxide could reach 80.6%. Moreover, the reaction mechanism of selective oxidation of styrene to styrene oxide using PcsM as a catalyst is reasonably proposed. Importantly, PcsM shows an excellent recyclable performance.

quote

GB/T 7714-2015 [1] Chenyu Sun, Hongzhi Liu. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00547.
MLA [1] Chenyu Sun, and Hongzhi Liu. ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00547.
APA [1] Chenyu Sun, & Hongzhi Liu. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00547
IEEE [1] Chenyu Sun and Hongzhi Liu, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00547. keywords: {silsesquioxane;porous polymer;styrene oxidation;heterogeneous catalysis;porphyrin}