Luminescence-Sensitive Surfaces Bearing Ratiometric Nanoparticles for Bacteria Growth Detection AITranslate
Abstract AITranslate
pH is one of the most fundamental parameters describing the quality of an aqueous solution. We developed a ratiometric fluorescent platform to monitor pH not only in solution but also on surfaces: our nanoprobe is based on fluorescent nanoparticles (FNPs) with a red-emitting BODIPY core and a pH-sensitive fluorescein derivative grafted on the outer shell. We demonstrated that a limited but controlled Förster resonance energy transfer occurs between two fluorophores. Such pH-sensitive and ratiometric FNPs could be grafted on a silanized glass surface, still permitting the measurement of pH with good sensitivity and allowing the monitoring of Escherichia coli growth through optical measurements in physiological pH range.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00549
Chinese Library Classification Number:
Citation Information:
pH is one of the most fundamental parameters describing the quality of an aqueous solution. We developed a ratiometric fluorescent platform to monitor pH not only in solution but also on surfaces: our nanoprobe is based on fluorescent nanoparticles (FNPs) with a red-emitting BODIPY core and a pH-sensitive fluorescein derivative grafted on the outer shell. We demonstrated that a limited but controlled Förster resonance energy transfer occurs between two fluorophores. Such pH-sensitive and ratiometric FNPs could be grafted on a silanized glass surface, still permitting the measurement of pH with good sensitivity and allowing the monitoring of Escherichia coli growth through optical measurements in physiological pH range.
quote
| GB/T 7714-2015 | [1] Miaobo Pan, Gabriela Morán Cruz, Chloé Grazon, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00549. |
| MLA | [1] Miaobo Pan, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00549. |
| APA | [1] Miaobo Pan, Gabriela Morán Cruz, Chloé Grazon, Djamila Kechkeche, Ludivine Houel Renault, Gilles Clavier, & Rachel MéalletRenault. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00549 |
| IEEE | [1] Miaobo Pan, Gabriela Morán Cruz, Chloé Grazon, Djamila Kechkeche, Ludivine Houel Renault, Gilles Clavier, and Rachel MéalletRenault, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00549. keywords: {polymer nanoparticle;fluorescent;ratiometric;pH measurement;glass surface} |