daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

3D Printability Assessment of Poly(octamethylene maleate (anhydride) citrate) and Poly(ethylene glycol) Diacrylate Copolymers for Biomedical Applications AITranslate

Institute of Global Health Innovation; Institute of Global Health Innovation; Imperial College London; Imperial College London
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Herein, we present the first example of 3D printing with poly(octamethylene maleate (anhydride) citrate) (POMaC), a bio-adhesive material which has shown particular promise for implantable biomedical devices. The current methods to fabricate such devices made from POMaC are hindered by the imposed constraints of designing complex molds. We demonstrate the feasibility of exploiting additive manufacturing to 3D print structural functional materials consisting of POMaC. We present 3D printing of biomaterial copolymers consisting of mixtures of poly(ethylene glycol) diacrylate (PEGDA) and POMaC at different ratios. The required parameters were optimized, and characterization of the printing fidelity and physical properties was performed. We have also demonstrated that a range of mechanical properties can be achieved by tuning the POMaC/PEGDA ratio. The biocompatibility of the copolymers was ascertained via a cell viability assay. Such tunable 3D printed biomaterials consisting of POMaC and PEGDA will have significant potential application in the development of functional biomaterial tissue scaffolds and biomedical devices for the future of personalized medicine.

KeyWords AITranslate

3D printing biomaterial tunable properties copolymers bioadhesion POMaC
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00531

Chinese Library Classification Number:

Citation Information:

Herein, we present the first example of 3D printing with poly(octamethylene maleate (anhydride) citrate) (POMaC), a bio-adhesive material which has shown particular promise for implantable biomedical devices. The current methods to fabricate such devices made from POMaC are hindered by the imposed constraints of designing complex molds. We demonstrate the feasibility of exploiting additive manufacturing to 3D print structural functional materials consisting of POMaC. We present 3D printing of biomaterial copolymers consisting of mixtures of poly(ethylene glycol) diacrylate (PEGDA) and POMaC at different ratios. The required parameters were optimized, and characterization of the printing fidelity and physical properties was performed. We have also demonstrated that a range of mechanical properties can be achieved by tuning the POMaC/PEGDA ratio. The biocompatibility of the copolymers was ascertained via a cell viability assay. Such tunable 3D printed biomaterials consisting of POMaC and PEGDA will have significant potential application in the development of functional biomaterial tissue scaffolds and biomedical devices for the future of personalized medicine.

quote

GB/T 7714-2015 [1] Dominic J. Wales, Meysam Keshavarz, Carmel Howe, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00531.
MLA [1] Dominic J. Wales, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00531.
APA [1] Dominic J. Wales, Meysam Keshavarz, Carmel Howe, & Eric Yeatman. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00531
IEEE [1] Dominic J. Wales, Meysam Keshavarz, Carmel Howe, and Eric Yeatman, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00531. keywords: {3D printing;biomaterial;tunable properties;copolymers;bioadhesion;POMaC}