Crown Ethers Enable Room-Temperature Synthesis of CsPbBr3 Quantum Dots for Light-Emitting Diodes AITranslate

Energy Research Institute at NTU (ERI@N); Nanyang Technological University; Nanyang Technological University;Energy Research Institute at NTU (ERI@N); Nanyang Technological University;Energy Research Institute at NTU (ERI@N); Nanyang Technological University; Nanyang Technological University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The synthesis of all-inorganic cesium lead halide perovskite quantum dots (QDs) typically requires high temperatures, stringent conditions, large quantities of surface ligands, and judicious purification steps to overcome ligand-induced charge injection barriers in optoelectronic devices. Low-temperature syntheses generally require lower ligand concentrations but are severely limited by the low solubility of the Cs precursor. We describe an innovative and general approach employing crown ethers under ambient conditions to overcome these solubility limitations. The crown ethers facilitate complete dissolution of the CsBr precursor, rendering CsPbBr3 QD inks practical for device fabrication. The resultant light-emitting diodes (LEDs) displayed bright green emission, with a current efficiency and external quantum efficiency of 9.22 cd A–1 and 2.64%, respectively. This represents the first LED based on CsPbBr3 QDs prepared at room temperature. Lastly, the crown ethers form core–shell structures, opening new avenues to exploit their strong coordination strength.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.7b01257

Chinese Library Classification Number:

Citation Information:

The synthesis of all-inorganic cesium lead halide perovskite quantum dots (QDs) typically requires high temperatures, stringent conditions, large quantities of surface ligands, and judicious purification steps to overcome ligand-induced charge injection barriers in optoelectronic devices. Low-temperature syntheses generally require lower ligand concentrations but are severely limited by the low solubility of the Cs precursor. We describe an innovative and general approach employing crown ethers under ambient conditions to overcome these solubility limitations. The crown ethers facilitate complete dissolution of the CsBr precursor, rendering CsPbBr3 QD inks practical for device fabrication. The resultant light-emitting diodes (LEDs) displayed bright green emission, with a current efficiency and external quantum efficiency of 9.22 cd A–1 and 2.64%, respectively. This represents the first LED based on CsPbBr3 QDs prepared at room temperature. Lastly, the crown ethers form core–shell structures, opening new avenues to exploit their strong coordination strength.

quote

GB/T 7714-2015 [1] Sjoerd A. Veldhuis, Yan Fong Ng, Riyas Ahmad, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.7b01257.
MLA [1] Sjoerd A. Veldhuis, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.7b01257.
APA [1] Sjoerd A. Veldhuis, Yan Fong Ng, Riyas Ahmad, Annalisa Bruno, Nur Fadilah Jamaludin, Bahulayan Damodaran, Nripan Mathews, & Subodh G. Mhaisalkar. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.7b01257
IEEE [1] Sjoerd A. Veldhuis, Yan Fong Ng, Riyas Ahmad, Annalisa Bruno, Nur Fadilah Jamaludin, Bahulayan Damodaran, Nripan Mathews, and Subodh G. Mhaisalkar, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.7b01257.