Real-Time Visualization of Active Species in a Single-Site Metal–Organic Framework Photocatalyst AITranslate
Abstract AITranslate
In this work, we report a new single-site photocatalyst (Co-Ru-UIO-67(bpy)) based on a metal–organic framework platform with incorporated molecular photosensitizer and catalyst. We show that this catalyst not only demonstrates exceptional activity for light-driven H2 production but also can be recycled without loss of activity. Using the combination of optical transient absorption spectroscopy and in situ X-ray absorption spectroscopy, we not only captured the key CoI intermediate species formed after ultrafast charge transfer from the incorporated photosensitizer but also identified the rate-limiting step in the catalytic cycle, providing insight into the catalysis mechanism of these single-site metal–organic framework photocatalysts.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b00062
Chinese Library Classification Number:
Citation Information:
In this work, we report a new single-site photocatalyst (Co-Ru-UIO-67(bpy)) based on a metal–organic framework platform with incorporated molecular photosensitizer and catalyst. We show that this catalyst not only demonstrates exceptional activity for light-driven H2 production but also can be recycled without loss of activity. Using the combination of optical transient absorption spectroscopy and in situ X-ray absorption spectroscopy, we not only captured the key CoI intermediate species formed after ultrafast charge transfer from the incorporated photosensitizer but also identified the rate-limiting step in the catalytic cycle, providing insight into the catalysis mechanism of these single-site metal–organic framework photocatalysts.
quote
| GB/T 7714-2015 | [1] Sizhuo Yang, Brian Pattengale, Sungsik Lee, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00062. |
| MLA | [1] Sizhuo Yang, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00062. |
| APA | [1] Sizhuo Yang, Brian Pattengale, Sungsik Lee, & Jier Huang. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00062 |
| IEEE | [1] Sizhuo Yang, Brian Pattengale, Sungsik Lee, and Jier Huang, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00062. |