Trimetallic NiFeMo for Overall Electrochemical Water Splitting with a Low Cell Voltage AITranslate

University of Houston; University of Houston; University of Houston; University of Houston; University of Houston; University of Houston; University of Houston; University of Houston; University of Electronic Science and Technology of China; University of Houston
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We report the development of an efficient and earth-abundant catalyst for electrochemical overall water splitting. Trimetallic NiFeMo alloy is synthesized by hydrothermal deposition from inorganic precursors and subsequent low-temperature thermal annealing. A complete cell made of NiFeMo electrodes on nickel foam exhibits a low voltage of 1.45 V at 10 mA/cm2 as a result of low overpotentials for both hydrogen evolution reaction (HER) and oxygen evolution reaction (OER). High-resolution transmission electron microscopy reveals that nanometer-sized single-crystal domains of Ni, Fe, and Mo are intimately integrated at the atomic level, which enables a synergistic effect of metallic Ni, Fe, and Mo for efficient HER, while self-formed Ni–Fe–Mo (oxy)hydroxides on the surface of the NiFeMo anode become active sites for OER. Such a multimetallic alloy and its (oxy)hydroxides represent a typical HER/OER catalyst couple, and our method provides a new route to develop efficient low-cost metallic alloys for overall water splitting.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.7b01335

Chinese Library Classification Number:

Citation Information:

We report the development of an efficient and earth-abundant catalyst for electrochemical overall water splitting. Trimetallic NiFeMo alloy is synthesized by hydrothermal deposition from inorganic precursors and subsequent low-temperature thermal annealing. A complete cell made of NiFeMo electrodes on nickel foam exhibits a low voltage of 1.45 V at 10 mA/cm2 as a result of low overpotentials for both hydrogen evolution reaction (HER) and oxygen evolution reaction (OER). High-resolution transmission electron microscopy reveals that nanometer-sized single-crystal domains of Ni, Fe, and Mo are intimately integrated at the atomic level, which enables a synergistic effect of metallic Ni, Fe, and Mo for efficient HER, while self-formed Ni–Fe–Mo (oxy)hydroxides on the surface of the NiFeMo anode become active sites for OER. Such a multimetallic alloy and its (oxy)hydroxides represent a typical HER/OER catalyst couple, and our method provides a new route to develop efficient low-cost metallic alloys for overall water splitting.

quote

GB/T 7714-2015 [1] Fan Qin, Zhenhuan Zhao, Md Kamrul Alam, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.7b01335.
MLA [1] Fan Qin, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.7b01335.
APA [1] Fan Qin, Zhenhuan Zhao, Md Kamrul Alam, Yizhou Ni, Francisco RoblesHernandez, Luo Yu, Shuo Chen, Zhifeng Ren, Zhiming Wang, & Jiming Bao. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.7b01335
IEEE [1] Fan Qin, Zhenhuan Zhao, Md Kamrul Alam, Yizhou Ni, Francisco RoblesHernandez, Luo Yu, Shuo Chen, Zhifeng Ren, Zhiming Wang, and Jiming Bao, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.7b01335.