The performance of asphalt mixtures greatly influences the long-term performance of bridge deck pavements. It is essential to optimise the asphalt mixtures with the best overall performance according to different regional conditions for use in engineering practice. This study proposes a comprehensive assessment method based on the Analytical Hierarchy Process (AHP) and Fuzzy Comprehensive Evaluation (FCE) to evaluate the serviceability of asphalt mixtures from different perspectives. It is used to optimise the best asphalt mixtures. The results show that the skeleton-dense structure asphalt mixture has better engineering applicability than the suspension-dense structure asphalt mixture, and the comprehensive performance of the asphalt mixture decreases with the increase of the nominal maximum particle size. The FCE determines that the total performance of the seven types of asphalt mixtures in the order of their superiority and inferiority are SMA-13 >asphalt mastic sand (AMS)>SMA-10 >AC-25 >AC-13 >AC-16 >AC-20. The study combines qualitative and quantitative factors, which makes the selection of engineering materials more scientific and rigorous and improves the rationality of material suitability evaluation.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.cscm.2023.e02784
Chinese Library Classification Number:
Citation Information:
The performance of asphalt mixtures greatly influences the long-term performance of bridge deck pavements. It is essential to optimise the asphalt mixtures with the best overall performance according to different regional conditions for use in engineering practice. This study proposes a comprehensive assessment method based on the Analytical Hierarchy Process (AHP) and Fuzzy Comprehensive Evaluation (FCE) to evaluate the serviceability of asphalt mixtures from different perspectives. It is used to optimise the best asphalt mixtures. The results show that the skeleton-dense structure asphalt mixture has better engineering applicability than the suspension-dense structure asphalt mixture, and the comprehensive performance of the asphalt mixture decreases with the increase of the nominal maximum particle size. The FCE determines that the total performance of the seven types of asphalt mixtures in the order of their superiority and inferiority are SMA-13 >asphalt mastic sand (AMS)>SMA-10 >AC-25 >AC-13 >AC-16 >AC-20. The study combines qualitative and quantitative factors, which makes the selection of engineering materials more scientific and rigorous and improves the rationality of material suitability evaluation.
quote
| GB/T 7714-2015 | [1] Xian Li, Jiancun Fu, Fei Yang, et al. Case Studies in Construction Materials, 2024(20). DOI:10.1016/j.cscm.2023.e02784. |
| MLA | [1] Xian Li, et al., Case Studies in Construction Materials, no. 20, 2024, https://doi.org/10.1016/j.cscm.2023.e02784. |
| APA | [1] Xian Li, Jiancun Fu, Fei Yang, HongLin Cao, Zhaojie Zhang, Fangtao Liu, Junrui Huang, & Yongfa Li. (2024). Case Studies in Construction Materials(20). https://doi.org/10.1016/j.cscm.2023.e02784 |
| IEEE | [1] Xian Li, Jiancun Fu, Fei Yang, HongLin Cao, Zhaojie Zhang, Fangtao Liu, Junrui Huang, and Yongfa Li, Case Studies in Construction Materials, no. 20, 2024, doi: 10.1016/j.cscm.2023.e02784. keywords: {Bridge deck pavement;Conventional asphalt mixtures;Fuzzy comprehensive evaluation (FCE);Pavement performance;Analytic hierarchy process (AHP)} |