daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Comparative analysis of dynamic mechanical properties of steel fiber reinforced concrete under ambient temperature and after exposure to high temperatures AITranslate

Beijing University of Technology; Beijing University of Technology; Shanghai Normal University; Beijing University of Technology; Beijing University of Technology; Beijing University of Technology
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The dynamic properties of concrete structures after being exposed to high temperatures play a crucial role in post-disaster repair and accident prevention measures. This study examined three different mixture ratios of Steel Fiber Reinforced Concrete (SFRC) with matrix strength of C60 and steel fiber contents of 0%, 1%, and 2%. A Split Hopkinson Pressure Bar (SHPB) with a diameter of 75 mm, along with a heating furnace, was employed to comprehensively investigate the dynamic compression behavior of materials. The specimens were exposed to temperatures ranging from 200 °C to 600 °C. In addition to evaluating the extent of mechanical degradation in SFRC after cooling, auxiliary impact experiments were also carried out at ambient temperature. The experimental data revealed that the dynamic peak stress and peak strain initially increased but eventually decreased as the loading rates continued to rise. The degree of strengthening, toughening, and energy absorption capacity of concrete materials progressively decreased as the escalation of strain rate after the cooling process. Moreover, the inclusion of steel fibers proved effective in preventing cracking and damage to the concrete, preserving the integrity of specimens even at higher temperatures. Simultaneously, the residual stress and deformation capacity of SFRC showed considerable enhancement after exposure to elevated temperatures.

KeyWords AITranslate

Steel Fiber Reinforced Concrete (SRFC) Dynamic compressive performance Split Hopkinson Pressure Bar (SHPB) Natural cooling after high temperatures Dynamic Increase Factor (DIF)
No data

Basic Information:

DOI:https://doi.org/10.1016/j.cscm.2023.e02778

Chinese Library Classification Number:

Citation Information:

The dynamic properties of concrete structures after being exposed to high temperatures play a crucial role in post-disaster repair and accident prevention measures. This study examined three different mixture ratios of Steel Fiber Reinforced Concrete (SFRC) with matrix strength of C60 and steel fiber contents of 0%, 1%, and 2%. A Split Hopkinson Pressure Bar (SHPB) with a diameter of 75 mm, along with a heating furnace, was employed to comprehensively investigate the dynamic compression behavior of materials. The specimens were exposed to temperatures ranging from 200 °C to 600 °C. In addition to evaluating the extent of mechanical degradation in SFRC after cooling, auxiliary impact experiments were also carried out at ambient temperature. The experimental data revealed that the dynamic peak stress and peak strain initially increased but eventually decreased as the loading rates continued to rise. The degree of strengthening, toughening, and energy absorption capacity of concrete materials progressively decreased as the escalation of strain rate after the cooling process. Moreover, the inclusion of steel fibers proved effective in preventing cracking and damage to the concrete, preserving the integrity of specimens even at higher temperatures. Simultaneously, the residual stress and deformation capacity of SFRC showed considerable enhancement after exposure to elevated temperatures.

quote

GB/T 7714-2015 [1] Liang Li, Zichen Wang, Jun Wu, et al. Case Studies in Construction Materials, 2024(20). DOI:10.1016/j.cscm.2023.e02778.
MLA [1] Liang Li, et al., Case Studies in Construction Materials, no. 20, 2024, https://doi.org/10.1016/j.cscm.2023.e02778.
APA [1] Liang Li, Zichen Wang, Jun Wu, Xiuli Du, Hongwei Wang, & Wenli Liu. (2024). Case Studies in Construction Materials(20). https://doi.org/10.1016/j.cscm.2023.e02778
IEEE [1] Liang Li, Zichen Wang, Jun Wu, Xiuli Du, Hongwei Wang, and Wenli Liu, Case Studies in Construction Materials, no. 20, 2024, doi: 10.1016/j.cscm.2023.e02778. keywords: {Steel Fiber Reinforced Concrete (SRFC);Dynamic compressive performance;Split Hopkinson Pressure Bar (SHPB);Natural cooling after high temperatures;Dynamic Increase Factor (DIF)}