Ultrastable 1T-2H WS2 Heterostructures by Nanoarchitectonics of Phosphorus-Triggered Phase Transition for Hybrid Supercapacitors AITranslate

National Institute for Materials Science (NIMS); Khalifa University; Dongguk University-Seoul; University of Sharjah; Khalifa University; Dongguk University-Seoul; Aston University; The University of Tokyo
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Tungsten disulfide (WS2) has recently emerged as a nontrivial material for electrochemical applications; however, boundaries associated with its 1T and 2H phases limit its performance. Here, this issue is addressed by evolving a dual-phase 1T-2H WS2 heterostructure that combines two different phases directly on the current collector. The resulting material demonstrated a 2D transformable phase structure, large interlayer distance, and highly exposed edge-active sites. Theoretical calculations confirmed that the 1T WS2 formed after phosphorus doping exhibits a semimetallic feature, elucidating a high electronic conductivity. The edge-enriched metallic phase and interlayer engineering of the 1T-2H WS2 heterostructure validate exceptional Na+ ion intercalation. The hybrid supercapacitor cell assembled with the 1T-2H WS2 anode and Prussian blue analogue (PBA) cathode shows a specific energy of 65.5 Wh kg–1 at 784 W kg–1, and 95.7% cycling stability. This work paves a technique for phase transition and sheds light on the expansion of efficient energy storage devices.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01452

Chinese Library Classification Number:

Citation Information:

Tungsten disulfide (WS2) has recently emerged as a nontrivial material for electrochemical applications; however, boundaries associated with its 1T and 2H phases limit its performance. Here, this issue is addressed by evolving a dual-phase 1T-2H WS2 heterostructure that combines two different phases directly on the current collector. The resulting material demonstrated a 2D transformable phase structure, large interlayer distance, and highly exposed edge-active sites. Theoretical calculations confirmed that the 1T WS2 formed after phosphorus doping exhibits a semimetallic feature, elucidating a high electronic conductivity. The edge-enriched metallic phase and interlayer engineering of the 1T-2H WS2 heterostructure validate exceptional Na+ ion intercalation. The hybrid supercapacitor cell assembled with the 1T-2H WS2 anode and Prussian blue analogue (PBA) cathode shows a specific energy of 65.5 Wh kg–1 at 784 W kg–1, and 95.7% cycling stability. This work paves a technique for phase transition and sheds light on the expansion of efficient energy storage devices.

quote

GB/T 7714-2015 [1] Pragati A. Shinde, Nilesh R. Chodankar, HyungJin Kim, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01452.
MLA [1] Pragati A. Shinde, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01452.
APA [1] Pragati A. Shinde, Nilesh R. Chodankar, HyungJin Kim, Mohammad Ali Abdelkareem, Amal Al Ghaferi, YoungKyu Han, Abdul Ghani Olabi, & Katsuhiko Ariga. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01452
IEEE [1] Pragati A. Shinde, Nilesh R. Chodankar, HyungJin Kim, Mohammad Ali Abdelkareem, Amal Al Ghaferi, YoungKyu Han, Abdul Ghani Olabi, and Katsuhiko Ariga, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01452.