daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A Perovskite Photovoltaic Mini-Module-CsPbBr3 Photoelectrochemical Cell Tandem Device for Solar-Driven Degradation of Organic Compounds AITranslate

Jeonbuk National University;Institute of Advanced Materials;Institute of Advanced Materials; Universidad Austral de Chile;Institute of Advanced Materials; Brno University of Technology;Institute of Advanced Materials; Jeonbuk National University;Institute of Advanced Materials
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Recently, halide perovskites have been widely explored for high-efficiency photocatalysis or photoelectrochemical (PEC) cells. Here, in order to make an efficient photoanode electrode for the degradation of pollutants, concretely 2-mercaptobenzothiazole (MBT), nanoscale cesium lead bromide (CsPbBr3) perovskite was directly formed on the surface of mesoporous titanium dioxide (meso-TiO2) film using a two-step spin-coating process. This photoelectrode recorded a photocurrent of up to 3.02 ± 0.03 mA/cm2 under standard AM 1.5G (100 mW/cm2) illumination through an optimization process such as introducing a thin aluminum oxide (Al2O3) coating layer. Furthermore, to supply high voltage for efficient oxidation of MBT without an external bias, we developed a new photovoltaic/PEC tandem system using a methylammonium lead iodide (MAPbI3) based mini-module consisting of three solar cells interconnected in series and confirmed its successful operation. This approach looks very promising due to its applicability to various PEC reactions.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01361

Chinese Library Classification Number:

Citation Information:

Recently, halide perovskites have been widely explored for high-efficiency photocatalysis or photoelectrochemical (PEC) cells. Here, in order to make an efficient photoanode electrode for the degradation of pollutants, concretely 2-mercaptobenzothiazole (MBT), nanoscale cesium lead bromide (CsPbBr3) perovskite was directly formed on the surface of mesoporous titanium dioxide (meso-TiO2) film using a two-step spin-coating process. This photoelectrode recorded a photocurrent of up to 3.02 ± 0.03 mA/cm2 under standard AM 1.5G (100 mW/cm2) illumination through an optimization process such as introducing a thin aluminum oxide (Al2O3) coating layer. Furthermore, to supply high voltage for efficient oxidation of MBT without an external bias, we developed a new photovoltaic/PEC tandem system using a methylammonium lead iodide (MAPbI3) based mini-module consisting of three solar cells interconnected in series and confirmed its successful operation. This approach looks very promising due to its applicability to various PEC reactions.

quote

GB/T 7714-2015 [1] SeulYi Lee, Patricio Serafini, Sofia Masi, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01361.
MLA [1] SeulYi Lee, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01361.
APA [1] SeulYi Lee, Patricio Serafini, Sofia Masi, Andrés F. GualdrónReyes, Camilo A. Mesa, Jhonatan RodríguezPereira, Sixto Giménez, Hyo Joong Lee, & Iván MoraSeró. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01361
IEEE [1] SeulYi Lee, Patricio Serafini, Sofia Masi, Andrés F. GualdrónReyes, Camilo A. Mesa, Jhonatan RodríguezPereira, Sixto Giménez, Hyo Joong Lee, and Iván MoraSeró, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01361.