High-Mobility and Bias-Stable Field-Effect Transistors Based on Lead-Free Formamidinium Tin Iodide Perovskites AITranslate

The Chinese University of Hong Kong; Eindhoven University of Technology; The Hong Kong University of Science and Technology; The Chinese University of Hong Kong; The Chinese University of Hong Kong; The Chinese University of Hong Kong; Eindhoven University of Technology; The Chinese University of Hong Kong
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Electronic devices based on tin halide perovskites often exhibit a poor operational stability. Here, we report an additive engineering strategy to realize high-performance and stable field-effect transistors (FETs) based on 3D formamidinium tin iodide (FASnI3) films. By comparatively studying the modification effects of two additives, i.e., phenethylammonium iodide and 4-fluorophenylethylammonium iodide via combined experimental and theoretical investigations, we unambiguously point out the general effects of phenethylammonium (PEA) and its fluorinated derivative (FPEA) in enhancing crystallization of FASnI3 films and the unique role of fluorination in reducing structural defects, suppressing oxidation of Sn2+ and blocking oxygen and water involved defect reactions. The optimized FPEA-modified FASnI3 FETs reach a record high field-effect mobility of 15.1 cm2/(V·s) while showing negligible hysteresis. The devices exhibit less than 10% and 3% current variation during over 2 h continuous bias stressing and 4200-cycle switching test, respectively, representing the best stability achieved so far for all Sn-based FETs.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01400

Chinese Library Classification Number:

Citation Information:

Electronic devices based on tin halide perovskites often exhibit a poor operational stability. Here, we report an additive engineering strategy to realize high-performance and stable field-effect transistors (FETs) based on 3D formamidinium tin iodide (FASnI3) films. By comparatively studying the modification effects of two additives, i.e., phenethylammonium iodide and 4-fluorophenylethylammonium iodide via combined experimental and theoretical investigations, we unambiguously point out the general effects of phenethylammonium (PEA) and its fluorinated derivative (FPEA) in enhancing crystallization of FASnI3 films and the unique role of fluorination in reducing structural defects, suppressing oxidation of Sn2+ and blocking oxygen and water involved defect reactions. The optimized FPEA-modified FASnI3 FETs reach a record high field-effect mobility of 15.1 cm2/(V·s) while showing negligible hysteresis. The devices exhibit less than 10% and 3% current variation during over 2 h continuous bias stressing and 4200-cycle switching test, respectively, representing the best stability achieved so far for all Sn-based FETs.

quote

GB/T 7714-2015 [1] Zhiwen Zhou, Qihua Li, Mojun Chen, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01400.
MLA [1] Zhiwen Zhou, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01400.
APA [1] Zhiwen Zhou, Qihua Li, Mojun Chen, Xuerong Zheng, Xiao Wu, Xinhui Lu, Shuxia Tao, & Ni Zhao. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01400
IEEE [1] Zhiwen Zhou, Qihua Li, Mojun Chen, Xuerong Zheng, Xiao Wu, Xinhui Lu, Shuxia Tao, and Ni Zhao, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01400.