Distal Synergistic Effect in Bimetal–Organic Framework for Superior Catalytic Water Oxidation AITranslate

Indian Institute of Science Education and Research; National Institute of Technology Karnataka; Indian Institute of Science Education and Research; Indian Institute of Science Education and Research; Indian Institute of Science Education and Research; Indian Institute of Science Education and Research; National Institute of Technology Karnataka; Indian Institute of Science Education and Research
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Metal–organic frameworks (MOFs) are emerging as promising electro-catalysts for the oxygen evolution reaction (OER). The bimetallic design strategy was further adopted in MOFs to elevate the OER performance by a synergistic effect. The proximal metal–oxygen–metal bonding configuration with typical 3dπ–2pπ–3dπ interaction was apparently essential for an effective electronic coupling between the metal centers. Here, we report an example of distal synergy in a bimetal–organic framework exhibiting a better OER activity than the monometallic counterparts, as well as the conventional proximal synergy. To achieve a current density of 10 mA·cm–2, our electrodeposited bimetallic MOF, Co–Ni(TCNQ)2(H2O)2 (TCNQ = 7,7,8,8-tetracyanoquinodimethane), on a glassy-carbon electrode required an overpotential value of 220 mV. X-ray photoelectron spectroscopy (XPS) and density functional theory (DFT) calculations revealed distinctive electronic coupling between the Co(II)-3d7 and Ni(II)-3d8 centers, despite being 9 Å apart, leading to an overall charge delocalization in the structure via TCNQ.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01626

Chinese Library Classification Number:

Citation Information:

Metal–organic frameworks (MOFs) are emerging as promising electro-catalysts for the oxygen evolution reaction (OER). The bimetallic design strategy was further adopted in MOFs to elevate the OER performance by a synergistic effect. The proximal metal–oxygen–metal bonding configuration with typical 3dπ–2pπ–3dπ interaction was apparently essential for an effective electronic coupling between the metal centers. Here, we report an example of distal synergy in a bimetal–organic framework exhibiting a better OER activity than the monometallic counterparts, as well as the conventional proximal synergy. To achieve a current density of 10 mA·cm–2, our electrodeposited bimetallic MOF, Co–Ni(TCNQ)2(H2O)2 (TCNQ = 7,7,8,8-tetracyanoquinodimethane), on a glassy-carbon electrode required an overpotential value of 220 mV. X-ray photoelectron spectroscopy (XPS) and density functional theory (DFT) calculations revealed distinctive electronic coupling between the Co(II)-3d7 and Ni(II)-3d8 centers, despite being 9 Å apart, leading to an overall charge delocalization in the structure via TCNQ.

quote

GB/T 7714-2015 [1] Umashis Bhoi, Subhasmita Ray, Sujit Bhand, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01626.
MLA [1] Umashis Bhoi, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01626.
APA [1] Umashis Bhoi, Subhasmita Ray, Sujit Bhand, Pranay Ninawe, Debashree Roy, Shammi Rana, Kartick Tarafder, & Nirmalya Ballav. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01626
IEEE [1] Umashis Bhoi, Subhasmita Ray, Sujit Bhand, Pranay Ninawe, Debashree Roy, Shammi Rana, Kartick Tarafder, and Nirmalya Ballav, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01626.