A Tetrathiafulvalene-based Bimetal–Organic Framework for a Hybrid Lithium-Ion Capacitor: The Role of Bimetallic Centers in Charge Storage and Stability AITranslate

Soochow University; Soochow University; Soochow University; Soochow University; Liaocheng University; Soochow University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Metal–organic frameworks (MOFs) have been found to be promising electrode materials for hybrid lithium-ion capacitors (HLICs) but face challenges due to their low capacity and cycling instability. Here, the first tetrathiafulvalene (TTF)-based bimetallic TTFTB-MnCo-MOF 1 was directly used as the electrode material for lithium-ion batteries, which presents enhanced performance compared with the isomorphic monometallic electrodes. Comprehensive characterizations reveal that Mn(II) in 1 is beneficial to the cycling stability and Co(II) contributes to the high specific capacity. The 1||NMC 622 full cell presents a capacity of 154.9 mAh g–1 at 100 mA g–1 in the 200th cycle. 1||AC HLIC displays a high specific energy of 141.4 Wh kg–1 at a specific power of 0.25 kW kg–1 and stable cycling performance. The remarkable performance, long-term cycling stability, and low self-discharge rate of the device are greater than those of most reported HLICs.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01677

Chinese Library Classification Number:

Citation Information:

Metal–organic frameworks (MOFs) have been found to be promising electrode materials for hybrid lithium-ion capacitors (HLICs) but face challenges due to their low capacity and cycling instability. Here, the first tetrathiafulvalene (TTF)-based bimetallic TTFTB-MnCo-MOF 1 was directly used as the electrode material for lithium-ion batteries, which presents enhanced performance compared with the isomorphic monometallic electrodes. Comprehensive characterizations reveal that Mn(II) in 1 is beneficial to the cycling stability and Co(II) contributes to the high specific capacity. The 1||NMC 622 full cell presents a capacity of 154.9 mAh g–1 at 100 mA g–1 in the 200th cycle. 1||AC HLIC displays a high specific energy of 141.4 Wh kg–1 at a specific power of 0.25 kW kg–1 and stable cycling performance. The remarkable performance, long-term cycling stability, and low self-discharge rate of the device are greater than those of most reported HLICs.

quote

GB/T 7714-2015 [1] LiJun Ma, ChenYue Luo, RuoNan Wang, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01677.
MLA [1] LiJun Ma, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01677.
APA [1] LiJun Ma, ChenYue Luo, RuoNan Wang, YuChuan Tan, JinLe Hou, & QinYu Zhu. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01677
IEEE [1] LiJun Ma, ChenYue Luo, RuoNan Wang, YuChuan Tan, JinLe Hou, and QinYu Zhu, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01677.