Tuning Surface Reactivity and Electric Field Strength via Intermetallic Alloying AITranslate
Abstract AITranslate
Many electrosynthesis reactions, such as CO2 reduction to multicarbon products, involve the formation of dipolar and polarizable transition states during the rate-determining step. Systematic and independent control over surface reactivity and electric field strength would accelerate the discovery of highly active electrocatalysts for these reactions by providing a means of reducing the transition state energy through field stabilization. Herein, we demonstrate that intermetallic alloying enables independent and systematic control over d-band energetics and work function through the variation of alloy composition and oxophilic constituent identity, respectively. We identify several intermetallic phases exhibiting properties that should collectively yield higher intrinsic activity for CO reduction compared to conventional Cu-based electrocatalysts. However, we also highlight the propensity of these alloys to segregate in air as a significant roadblock to investigating their electrocatalytic activity.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.3c01639
Chinese Library Classification Number:
Citation Information:
Many electrosynthesis reactions, such as CO2 reduction to multicarbon products, involve the formation of dipolar and polarizable transition states during the rate-determining step. Systematic and independent control over surface reactivity and electric field strength would accelerate the discovery of highly active electrocatalysts for these reactions by providing a means of reducing the transition state energy through field stabilization. Herein, we demonstrate that intermetallic alloying enables independent and systematic control over d-band energetics and work function through the variation of alloy composition and oxophilic constituent identity, respectively. We identify several intermetallic phases exhibiting properties that should collectively yield higher intrinsic activity for CO reduction compared to conventional Cu-based electrocatalysts. However, we also highlight the propensity of these alloys to segregate in air as a significant roadblock to investigating their electrocatalytic activity.
quote
| GB/T 7714-2015 | [1] Ezra L. Clark, Rasmus Nielsen, Jakob Ejler Sørensen, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01639. |
| MLA | [1] Ezra L. Clark, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01639. |
| APA | [1] Ezra L. Clark, Rasmus Nielsen, Jakob Ejler Sørensen, Julius Lucas Needham, Brian Seger, & Ib Chorkendorff. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01639 |
| IEEE | [1] Ezra L. Clark, Rasmus Nielsen, Jakob Ejler Sørensen, Julius Lucas Needham, Brian Seger, and Ib Chorkendorff, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01639. |