daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Stable and Exclusive Formation of CO from CO2 Photoreduction with H2O Facilitated by Linear Fluorene and Naphthalene Diimide-Based Conjugated Polymers AITranslate

National Taiwan University; National Taiwan University; National Taiwan University; National Taiwan University; National Taiwan University; National Taiwan University; National Taiwan University; National Taiwan University; National Taiwan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Five conjugated polymers are synthesized, characterized, and examined in heterogeneous CO2 photoreduction with H2O. A promising CO production rate of 10.07 μmol g–1 h–1 is achieved with exclusive formation of CO in the absence of amine sacrificial agents. This photocatalytic system is highly stable. No significant degradation in the CO production rate is observed after 104 h of illumination. The physical and photocatalytic properties of the polymers are compared, revealing that the lowest unoccupied molecular-orbital energy could be the most significant factor in determining the conversion efficiency. On the other hand, CO2 might be trapped by the tetraalkylammonium bromide functionality installed in a polymer, hampering CO generation. The presence of water vapor improves the CO production rate. Density functional theory (DFT) calculations indicate that water molecules can reduce the Gibbs free energy difference for CO2 reduction to CO. This work demonstrates the use of linear conjugated polymers in the CO2 photoreduction and illuminates the working principles, paving the way for conversion of solar energy into useful fuels.

KeyWords AITranslate

linear conjugated polymers CO2 photoreduction CO generation high stability high selectivity fluorene naphthalene diimide
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01419

Chinese Library Classification Number:

Citation Information:

Five conjugated polymers are synthesized, characterized, and examined in heterogeneous CO2 photoreduction with H2O. A promising CO production rate of 10.07 μmol g–1 h–1 is achieved with exclusive formation of CO in the absence of amine sacrificial agents. This photocatalytic system is highly stable. No significant degradation in the CO production rate is observed after 104 h of illumination. The physical and photocatalytic properties of the polymers are compared, revealing that the lowest unoccupied molecular-orbital energy could be the most significant factor in determining the conversion efficiency. On the other hand, CO2 might be trapped by the tetraalkylammonium bromide functionality installed in a polymer, hampering CO generation. The presence of water vapor improves the CO production rate. Density functional theory (DFT) calculations indicate that water molecules can reduce the Gibbs free energy difference for CO2 reduction to CO. This work demonstrates the use of linear conjugated polymers in the CO2 photoreduction and illuminates the working principles, paving the way for conversion of solar energy into useful fuels.

quote

GB/T 7714-2015 [1] WeiChun Lai, ShihHao Wang, HanSheng Sun, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01419.
MLA [1] WeiChun Lai, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01419.
APA [1] WeiChun Lai, ShihHao Wang, HanSheng Sun, CheWei Liao, TaoYuan Liu, HaoTing Lee, HauRen Yang, Leeyih Wang, & YuYing Lai. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01419
IEEE [1] WeiChun Lai, ShihHao Wang, HanSheng Sun, CheWei Liao, TaoYuan Liu, HaoTing Lee, HauRen Yang, Leeyih Wang, and YuYing Lai, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01419. keywords: {linear conjugated polymers;CO2 photoreduction;CO generation;high stability;high selectivity;fluorene;naphthalene diimide}