Organic–Inorganic Polyureas with POSS Cages in the Main Chains via Polycondensation of Diamines with Carbon Dioxide AITranslate

Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Linear organic–inorganic polyureas (PUreas) with polyhedral oligomeric silsesquioxane (POSS) cages in the main chains were synthesized via polycondensation of diamines with carbon dioxide (CO2). First, 3,13-dianilino double decker silsesquioxane (denoted 3,13-dianilino DDSQ) was synthesized. An α,ω-diamino-terminated poly(propylene oxide) as well as the POSS diamine was exploited for polycondensation with CO2; PUrea and PUrea-DDSQ with sufficiently high molecular weights were obtained with various contents of POSS. The morphological investigation shows that the linear PUreas with POSS cages in the main chains were microphase-separated; the POSS cages were aggregated into spherical microdomains with the size of 50–120 nm in diameter. Owing to the introduction of POSS cages, PUrea was transformed from a viscous liquid into elastic solids in the ranges of composition investigated. At room temperature, linear organic–inorganic PUreas behaved as cross-linked elastomers. This behavior is ascribed to the generation of physical cross-linking with POSS microdomains as the cross-linking sites. In addition, the organic–inorganic PUreas displayed self-healing properties via the dynamic exchange of multiple hydrogen bonds. It was found that the self-healing properties were significantly affected by the content of 3,13-dianilino DDSQ.

KeyWords AITranslate

PUreas carbon dioxide diamine POSS selfhealing properties
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01399

Chinese Library Classification Number:

Citation Information:

Linear organic–inorganic polyureas (PUreas) with polyhedral oligomeric silsesquioxane (POSS) cages in the main chains were synthesized via polycondensation of diamines with carbon dioxide (CO2). First, 3,13-dianilino double decker silsesquioxane (denoted 3,13-dianilino DDSQ) was synthesized. An α,ω-diamino-terminated poly(propylene oxide) as well as the POSS diamine was exploited for polycondensation with CO2; PUrea and PUrea-DDSQ with sufficiently high molecular weights were obtained with various contents of POSS. The morphological investigation shows that the linear PUreas with POSS cages in the main chains were microphase-separated; the POSS cages were aggregated into spherical microdomains with the size of 50–120 nm in diameter. Owing to the introduction of POSS cages, PUrea was transformed from a viscous liquid into elastic solids in the ranges of composition investigated. At room temperature, linear organic–inorganic PUreas behaved as cross-linked elastomers. This behavior is ascribed to the generation of physical cross-linking with POSS microdomains as the cross-linking sites. In addition, the organic–inorganic PUreas displayed self-healing properties via the dynamic exchange of multiple hydrogen bonds. It was found that the self-healing properties were significantly affected by the content of 3,13-dianilino DDSQ.

quote

GB/T 7714-2015 [1] Bingjie Zhao, Honggang Mei, Huaming Wang, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01399.
MLA [1] Bingjie Zhao, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01399.
APA [1] Bingjie Zhao, Honggang Mei, Huaming Wang, Lei Li, & Sixun Zheng. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01399
IEEE [1] Bingjie Zhao, Honggang Mei, Huaming Wang, Lei Li, and Sixun Zheng, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01399. keywords: {PUreas;carbon dioxide;diamine;POSS;selfhealing properties}