daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Above 600 mV Open-Circuit Voltage BiI3 Solar Cells AITranslate

University of Bristol; University Walk; University of Bristol
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Phase-pure BiI3 films obtained by versatile gas-phase iodination of Bi2S3 are investigated as an absorber in photovoltaic devices. This preparation method leads to highly crystalline BiI3 films featuring a rhombohedral phase and a high-degree of stacking order. The films are composed of micrometer-sized flat grains distributed homogeneously across the F-doped SnO2 (FTO) substrate, exhibiting an indirect band gap transition at 1.72 eV. High-level calculations based on G0W0 approximation are used to rationalize the electronic structure of BiI3, confirming the band gap value estimated experimentally. The films show p-type conductivity with an acceptor density on the order of 1015 cm–3. Solar cells with the architecture glass/FTO/TiO2/BiI3/F8/Au, where F8 is poly(9,9-di-n-octylfluorenyl-2,7-diyl), display a record open-circuit voltage above 600 mV and overall power conversion efficiency of 1.2% under AM 1.5G illumination. The large open-circuit potential is rationalized in terms of carrier lifetimes longer than 1 ns as probed by time-resolved photoluminescence spectroscopy.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01182

Chinese Library Classification Number:

Citation Information:

Phase-pure BiI3 films obtained by versatile gas-phase iodination of Bi2S3 are investigated as an absorber in photovoltaic devices. This preparation method leads to highly crystalline BiI3 films featuring a rhombohedral phase and a high-degree of stacking order. The films are composed of micrometer-sized flat grains distributed homogeneously across the F-doped SnO2 (FTO) substrate, exhibiting an indirect band gap transition at 1.72 eV. High-level calculations based on G0W0 approximation are used to rationalize the electronic structure of BiI3, confirming the band gap value estimated experimentally. The films show p-type conductivity with an acceptor density on the order of 1015 cm–3. Solar cells with the architecture glass/FTO/TiO2/BiI3/F8/Au, where F8 is poly(9,9-di-n-octylfluorenyl-2,7-diyl), display a record open-circuit voltage above 600 mV and overall power conversion efficiency of 1.2% under AM 1.5G illumination. The large open-circuit potential is rationalized in terms of carrier lifetimes longer than 1 ns as probed by time-resolved photoluminescence spectroscopy.

quote

GB/T 7714-2015 [1] Devendra Tiwari, Dominic Alibhai, David J Fermin. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01182.
MLA [1] Devendra Tiwari, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01182.
APA [1] Devendra Tiwari, Dominic Alibhai, & David J Fermin. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01182
IEEE [1] Devendra Tiwari, Dominic Alibhai, and David J Fermin, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01182.