daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Over 1% Efficient Unbiased Stable Solar Water Splitting Based on a Sprayed Cu2ZnSnS4 Photocathode Protected by a HfO2 Photocorrosion-Resistant Film AITranslate

South China Normal University; South China Normal University; South China Normal University; Osaka University; Konan University; South China Normal University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Surface passivation of the CdS/Cu2ZnSnS4 photocathode by a HfO2 layer was found to be very effective for enhancing the photoelectrochemical stability. The dependence of the photoelectrochemical performance, especially the stability of the Cu2ZnSnS4-based photocathode, on the thickness of the HfO2 film was systematically investigated. The thickness of the HfO2 layer obviously influenced the PEC stability and efficiency of the Cu2ZnSnS4-based photocathode. The CdS/Cu2ZnSnS4 photocathode modified with a 6 nm thick HfO2 layer showed long-term PEC photocurrent stability of over 10 h while still retaining high half-cell solar-to-hydrogen efficiency (HC-STH) of 2.7%. Finally, we fabricated an unbiased solar water splitting device based on the Pt/HfO2/CdS/Cu2ZnSnS4 photocathode in tandem with a BiVO4 photoanode, and this tandem device not only exhibited an unassisted STH conversion efficiency of 1.046% but also showed a high long-term stability of over 10 h.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01005

Chinese Library Classification Number:

Citation Information:

Surface passivation of the CdS/Cu2ZnSnS4 photocathode by a HfO2 layer was found to be very effective for enhancing the photoelectrochemical stability. The dependence of the photoelectrochemical performance, especially the stability of the Cu2ZnSnS4-based photocathode, on the thickness of the HfO2 film was systematically investigated. The thickness of the HfO2 layer obviously influenced the PEC stability and efficiency of the Cu2ZnSnS4-based photocathode. The CdS/Cu2ZnSnS4 photocathode modified with a 6 nm thick HfO2 layer showed long-term PEC photocurrent stability of over 10 h while still retaining high half-cell solar-to-hydrogen efficiency (HC-STH) of 2.7%. Finally, we fabricated an unbiased solar water splitting device based on the Pt/HfO2/CdS/Cu2ZnSnS4 photocathode in tandem with a BiVO4 photoanode, and this tandem device not only exhibited an unassisted STH conversion efficiency of 1.046% but also showed a high long-term stability of over 10 h.

quote

GB/T 7714-2015 [1] Dingwang Huang, Kang Wang, Le Yu, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01005.
MLA [1] Dingwang Huang, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01005.
APA [1] Dingwang Huang, Kang Wang, Le Yu, Thi Hiep Nguyen, Shigeru Ikeda, & Feng Jiang. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01005
IEEE [1] Dingwang Huang, Kang Wang, Le Yu, Thi Hiep Nguyen, Shigeru Ikeda, and Feng Jiang, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01005.