Photocatalytic Hydrogen Evolution from Substoichiometric Colloidal WO3–x Nanowires AITranslate

Chung-Ang University; Stanford University; University of Pennsylvania; University of Pennsylvania; University of Pennsylvania; University of Pennsylvania; Chung-Ang University; Korea University; University of Pennsylvania; University of Trieste; University of Pennsylvania
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We report direct photocatalytic hydrogen evolution from substoichiometric highly reduced tungsten oxide (WOx) nanowires (NWs) using sacrificial alcohol. WOx NWs are synthesized via nonaqueous colloidal synthesis with a diameter of about 4 nm and an average length of about 250 nm. As-synthesized WOx NWs exhibit a broad absorption across the visible to infrared regions attributed to the presence of oxygen vacancies. The optical band gap is increased in these WOx NWs compared to stoichiometric bulk tungsten oxide (WO3) powders as a result of the Burstein–Moss shift. As a consequence of this increase, we demonstrate direct photocatalytic hydrogen production from WOx NWs through alcohol photoreforming. The stable H2 evolution on platinized WOx NWs is observed under conditions in which platinized bulk WO3 and bulk WO2.9 powders either do not show activity or show very low rates, suggesting that increased surface area and specific exposed facets are key for the improved performance of WOx NWs. This work demonstrates that control of size and composition can lead to unexpected and beneficial changes in the photocatalytic properties of semiconductor materials.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b00925

Chinese Library Classification Number:

Citation Information:

We report direct photocatalytic hydrogen evolution from substoichiometric highly reduced tungsten oxide (WOx) nanowires (NWs) using sacrificial alcohol. WOx NWs are synthesized via nonaqueous colloidal synthesis with a diameter of about 4 nm and an average length of about 250 nm. As-synthesized WOx NWs exhibit a broad absorption across the visible to infrared regions attributed to the presence of oxygen vacancies. The optical band gap is increased in these WOx NWs compared to stoichiometric bulk tungsten oxide (WO3) powders as a result of the Burstein–Moss shift. As a consequence of this increase, we demonstrate direct photocatalytic hydrogen production from WOx NWs through alcohol photoreforming. The stable H2 evolution on platinized WOx NWs is observed under conditions in which platinized bulk WO3 and bulk WO2.9 powders either do not show activity or show very low rates, suggesting that increased surface area and specific exposed facets are key for the improved performance of WOx NWs. This work demonstrates that control of size and composition can lead to unexpected and beneficial changes in the photocatalytic properties of semiconductor materials.

quote

GB/T 7714-2015 [1] Taejong Paik, Matteo Cargnello, Thomas R. Gordon, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00925.
MLA [1] Taejong Paik, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00925.
APA [1] Taejong Paik, Matteo Cargnello, Thomas R. Gordon, Sen Zhang, Hongseok Yun, Jennifer D. Lee, Ho Young Woo, Soong Ju Oh, Cherie R. Kagan, Paolo Fornasiero, & Christopher B. Murray. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00925
IEEE [1] Taejong Paik, Matteo Cargnello, Thomas R. Gordon, Sen Zhang, Hongseok Yun, Jennifer D. Lee, Ho Young Woo, Soong Ju Oh, Cherie R. Kagan, Paolo Fornasiero, and Christopher B. Murray, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00925.