daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Improving Electrocatalysts for Oxygen Evolution Using NixFe3–xO4/Ni Hybrid Nanostructures Formed by Solvothermal Synthesis AITranslate

Harbin Institute of Technology; Harbin Institute of Technology; Harbin Institute of Technology; Harbin Institute of Technology; Harbin Institute of Technology; Harbin Institute of Technology; Dalian Jiaotong University; Harbin Institute of Technology; Taizhou University; 1101 University Avenue
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Spinel-type oxides have been found to be active electrocatalysts for OER. However, their semiconductor character severely limits their catalytic performance. Herein, we report a facile solvothermal pathway for the synthesis of spinel-type NixFe3–xO4 oxides/Ni metal nanocomposites. The good electrical contact between the metal and semiconductor oxide interface and well-tuned compositions of NixFe3–xO4 spinel oxides are crucial to achieve better OER performance. Specifically, the NixFe3–xO4/Ni nanocomposite sample prepared from a metal precursor ratio of y = 0.15 [y = Fe/(Fe + Ni)] that results in an x value of about 0.36 exhibits catalytic activity with an overpotential of 225 mV to achieve an electrocatalytic current density of j = 10 mA cm–2 and a Tafel slope of 44 mV dec–1 in alkaline electrolyte. This study not only provides new perspectives to designing nanocomposite catalysts for OER but also opens a promising avenue for further enhancing electrocatalytic performance via interface and composition engineering.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b00888

Chinese Library Classification Number:

Citation Information:

Spinel-type oxides have been found to be active electrocatalysts for OER. However, their semiconductor character severely limits their catalytic performance. Herein, we report a facile solvothermal pathway for the synthesis of spinel-type NixFe3–xO4 oxides/Ni metal nanocomposites. The good electrical contact between the metal and semiconductor oxide interface and well-tuned compositions of NixFe3–xO4 spinel oxides are crucial to achieve better OER performance. Specifically, the NixFe3–xO4/Ni nanocomposite sample prepared from a metal precursor ratio of y = 0.15 [y = Fe/(Fe + Ni)] that results in an x value of about 0.36 exhibits catalytic activity with an overpotential of 225 mV to achieve an electrocatalytic current density of j = 10 mA cm–2 and a Tafel slope of 44 mV dec–1 in alkaline electrolyte. This study not only provides new perspectives to designing nanocomposite catalysts for OER but also opens a promising avenue for further enhancing electrocatalytic performance via interface and composition engineering.

quote

GB/T 7714-2015 [1] Jinzhen Huang, Jiecai Han, Ran Wang, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00888.
MLA [1] Jinzhen Huang, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00888.
APA [1] Jinzhen Huang, Jiecai Han, Ran Wang, Yuanyuan Zhang, Xianjie Wang, Xinghong Zhang, Zhihua Zhang, Yumin Zhang, Bo Song, & Song Jin. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00888
IEEE [1] Jinzhen Huang, Jiecai Han, Ran Wang, Yuanyuan Zhang, Xianjie Wang, Xinghong Zhang, Zhihua Zhang, Yumin Zhang, Bo Song, and Song Jin, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00888.