Bilayer Chlorophyll-Based Biosolar Cells Inspired from the Z-Scheme Process of Oxygenic Photosynthesis AITranslate
Abstract AITranslate
The Z-scheme process in chlorophyll-based natural photosynthesis shows the pathway of photoinduced electron transport from photosystem II (PSII) to photosystem I (PSI) through an electron transfer chain. Inspired by the interesting Z-scheme of oxygenic photosynthesis, we imitated the dual photosynthesis systems into biosolar cells (BSCs). The device structure fabricated here is ITO/ZnO/Chl-A/Chl-D1, -D2, -D3, or -D4 (Chl-Ds)/MoO3/Ag. Due to higher HOMO/LUMO energy levels of Chl-A than those of Chl-Ds, the sublayer Chl-A corresponds to PSI, and the upper layer Chl-Ds are equivalent to PSII, leading to double photoexcited electron transfer from Chl-Ds to Chl-A. The energy alignment of the photoactive layers here is in conflict with the traditional comprehension of photovoltaic devices. Interestingly, such an uncommon device can still work well. A power conversion efficiency of 1.30% was reached based on the Chl-A/Chl-D4 device under standard AM1.5 illumination.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b00797
Chinese Library Classification Number:
Citation Information:
The Z-scheme process in chlorophyll-based natural photosynthesis shows the pathway of photoinduced electron transport from photosystem II (PSII) to photosystem I (PSI) through an electron transfer chain. Inspired by the interesting Z-scheme of oxygenic photosynthesis, we imitated the dual photosynthesis systems into biosolar cells (BSCs). The device structure fabricated here is ITO/ZnO/Chl-A/Chl-D1, -D2, -D3, or -D4 (Chl-Ds)/MoO3/Ag. Due to higher HOMO/LUMO energy levels of Chl-A than those of Chl-Ds, the sublayer Chl-A corresponds to PSI, and the upper layer Chl-Ds are equivalent to PSII, leading to double photoexcited electron transfer from Chl-Ds to Chl-A. The energy alignment of the photoactive layers here is in conflict with the traditional comprehension of photovoltaic devices. Interestingly, such an uncommon device can still work well. A power conversion efficiency of 1.30% was reached based on the Chl-A/Chl-D4 device under standard AM1.5 illumination.
quote
| GB/T 7714-2015 | [1] Shengnan Duan, Chunxiang Dall’Agnese, Gang Chen, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00797. |
| MLA | [1] Shengnan Duan, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00797. |
| APA | [1] Shengnan Duan, Chunxiang Dall’Agnese, Gang Chen, XiaoFeng Wang, Hitoshi Tamiaki, Yuya Yamamoto, Toshitaka Ikeuchi, & Shinichi Sasaki. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00797 |
| IEEE | [1] Shengnan Duan, Chunxiang Dall’Agnese, Gang Chen, XiaoFeng Wang, Hitoshi Tamiaki, Yuya Yamamoto, Toshitaka Ikeuchi, and Shinichi Sasaki, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00797. |