Role of Polarons in Water Splitting: The Case of BiVO4 AITranslate
Abstract AITranslate
We study hole and electron polarons in BiVO4 at finite temperature through hybrid functional molecular dynamics simulations. Through the thermodynamic integration method, we obtain the transition levels corresponding to the localized charges at 300 K. We observe that the polaron levels achieved in this way lie significantly closer to each other than those at 0 K. We find both hole and electron levels to lie within the band gap, with binding energies of 0.11 and 0.88 eV, respectively. Our calculations show that polaron localization significantly affects the alignment at the solid/liquid interface and that electron–hole recombination through polaronic states competes with the evolution of the water-splitting reaction in BiVO4.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b00938
Chinese Library Classification Number:
Citation Information:
We study hole and electron polarons in BiVO4 at finite temperature through hybrid functional molecular dynamics simulations. Through the thermodynamic integration method, we obtain the transition levels corresponding to the localized charges at 300 K. We observe that the polaron levels achieved in this way lie significantly closer to each other than those at 0 K. We find both hole and electron levels to lie within the band gap, with binding energies of 0.11 and 0.88 eV, respectively. Our calculations show that polaron localization significantly affects the alignment at the solid/liquid interface and that electron–hole recombination through polaronic states competes with the evolution of the water-splitting reaction in BiVO4.
quote
| GB/T 7714-2015 | [1] Julia Wiktor, Francesco Ambrosio, Alfredo Pasquarello. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00938. |
| MLA | [1] Julia Wiktor, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00938. |
| APA | [1] Julia Wiktor, Francesco Ambrosio, & Alfredo Pasquarello. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00938 |
| IEEE | [1] Julia Wiktor, Francesco Ambrosio, and Alfredo Pasquarello, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00938. |