On the True Composition of Mixed-Cation Perovskite Films AITranslate

Universidad Nacional Autónoma de México; Universidad Nacional Autónoma de México; Universidad Nacional Autónoma de México; Universidad Nacional Autónoma de México; Universidad Nacional Autónoma de México
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Herein we show that mixed-cation perovskite films made by spin-coating do not necessarily have the same stoichiometry as the precursor solution from which they are made and propose a simple method to quantify the true composition of such films.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01577

Chinese Library Classification Number:

Citation Information:

Herein we show that mixed-cation perovskite films made by spin-coating do not necessarily have the same stoichiometry as the precursor solution from which they are made and propose a simple method to quantify the true composition of such films.

quote

GB/T 7714-2015 [1] Carina ParejaRivera, Ana L. SolísCambero, Mireille SánchezTorres, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01577.
MLA [1] Carina ParejaRivera, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01577.
APA [1] Carina ParejaRivera, Ana L. SolísCambero, Mireille SánchezTorres, Enrique Lima, & Diego SolisIbarra. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01577
IEEE [1] Carina ParejaRivera, Ana L. SolísCambero, Mireille SánchezTorres, Enrique Lima, and Diego SolisIbarra, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01577.