Stability at Scale: Challenges of Module Interconnects for Perovskite Photovoltaics AITranslate
Publisher: ACS
Abstract AITranslate
Uniting efficiency, scalability, and stability is the next frontier for perovskite solar cells. Stability tests conducted on efficient perovskite solar cell mini-module architectures reveal promising stability yet also the stability challenges of scale up.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b01498
Chinese Library Classification Number:
Citation Information:
Uniting efficiency, scalability, and stability is the next frontier for perovskite solar cells. Stability tests conducted on efficient perovskite solar cell mini-module architectures reveal promising stability yet also the stability challenges of scale up.
quote
| GB/T 7714-2015 | [1] Jeffrey A. Christians, Fei Zhang, Rosemary C. Bramante, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01498. |
| MLA | [1] Jeffrey A. Christians, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01498. |
| APA | [1] Jeffrey A. Christians, Fei Zhang, Rosemary C. Bramante, Matthew O. Reese, Tracy H. Schloemer, Alan Sellinger, Maikel F. A. M. van Hest, Kai Zhu, Joseph J. Berry, & Joseph M. Luther. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01498 |
| IEEE | [1] Jeffrey A. Christians, Fei Zhang, Rosemary C. Bramante, Matthew O. Reese, Tracy H. Schloemer, Alan Sellinger, Maikel F. A. M. van Hest, Kai Zhu, Joseph J. Berry, and Joseph M. Luther, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01498. |