Present and Future Perspective on Electrode Materials for Rechargeable Zinc-Ion Batteries AITranslate
Abstract AITranslate
The zinc-ion battery (ZIB) is a 2 century-old technology but has recently attracted renewed interest owing to the possibility of switching from primary to rechargeable ZIBs. Nowadays, ZIBs employing a mild aqueous electrolyte are considered one of the most promising candidates for emerging energy storage systems (ESS) and portable electronics applications due to their environmental friendliness, safety, low cost, and acceptable energy density. However, there are many drawbacks associated with these batteries that have not yet been resolved. In this Review, we present the challenges and recent developments related to rechargeable ZIB research. Recent research trends and directions on electrode materials that can store Zn2+ and electrolytes that can improve the battery performance are comprehensively discussed.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b01552
Chinese Library Classification Number:
Citation Information:
The zinc-ion battery (ZIB) is a 2 century-old technology but has recently attracted renewed interest owing to the possibility of switching from primary to rechargeable ZIBs. Nowadays, ZIBs employing a mild aqueous electrolyte are considered one of the most promising candidates for emerging energy storage systems (ESS) and portable electronics applications due to their environmental friendliness, safety, low cost, and acceptable energy density. However, there are many drawbacks associated with these batteries that have not yet been resolved. In this Review, we present the challenges and recent developments related to rechargeable ZIB research. Recent research trends and directions on electrode materials that can store Zn2+ and electrolytes that can improve the battery performance are comprehensively discussed.
quote
| GB/T 7714-2015 | [1] Aishuak Konarov, Natalia Voronina, Jae Hyeon Jo, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01552. |
| MLA | [1] Aishuak Konarov, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01552. |
| APA | [1] Aishuak Konarov, Natalia Voronina, Jae Hyeon Jo, Zhumabay Bakenov, YangKook Sun, & SeungTaek Myung. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01552 |
| IEEE | [1] Aishuak Konarov, Natalia Voronina, Jae Hyeon Jo, Zhumabay Bakenov, YangKook Sun, and SeungTaek Myung, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01552. |