Surface-Initiated Controlled Radical Polymerization: Going beyond Laboratory Scale AITranslate
Abstract AITranslate
Surface coatings of immobilized polymer brushes are used, e.g., as lubricants, for anti-fouling, and as adhesives. Based on surface-initiated controlled radical polymerization (SI-CRP), a fast, versatile, and enduring scaled SI-CRP (SI-CRPscaled) approach for the formation of polymer brushes is reported. The chemical process is made from an easily prepared chemical solution that is reusable for more than 6 h, even in the presence of oxygen. Because an inert atmosphere is not required, the SI-CRPscaled process can be carried out under ambient conditions with no significant loss of polymerization activity and viability. The high bath life of the activated solution along with an extraordinarily high brush growth rate of 10 nm per minute makes this method industrially relevant. Based on a straightforward dip coating protocol, this is the first scaled polymer brush technique successfully demonstrated on an industrial scale, enabling uniform polymer brush-functionalized materials for a broader variety of applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c00205
Chinese Library Classification Number:
Citation Information:
Surface coatings of immobilized polymer brushes are used, e.g., as lubricants, for anti-fouling, and as adhesives. Based on surface-initiated controlled radical polymerization (SI-CRP), a fast, versatile, and enduring scaled SI-CRP (SI-CRPscaled) approach for the formation of polymer brushes is reported. The chemical process is made from an easily prepared chemical solution that is reusable for more than 6 h, even in the presence of oxygen. Because an inert atmosphere is not required, the SI-CRPscaled process can be carried out under ambient conditions with no significant loss of polymerization activity and viability. The high bath life of the activated solution along with an extraordinarily high brush growth rate of 10 nm per minute makes this method industrially relevant. Based on a straightforward dip coating protocol, this is the first scaled polymer brush technique successfully demonstrated on an industrial scale, enabling uniform polymer brush-functionalized materials for a broader variety of applications.
quote
| GB/T 7714-2015 | [1] Jakob Pagh Nikolajsen, Lukas Vogtmann Thinnesen, Orhan Altuğ Karabiber, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00205. |
| MLA | [1] Jakob Pagh Nikolajsen, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00205. |
| APA | [1] Jakob Pagh Nikolajsen, Lukas Vogtmann Thinnesen, Orhan Altuğ Karabiber, Kim Daasbjerg, Steen Uttrup Pedersen, Mikkel Kongsfelt, & Mie Lillethorup. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00205 |
| IEEE | [1] Jakob Pagh Nikolajsen, Lukas Vogtmann Thinnesen, Orhan Altuğ Karabiber, Kim Daasbjerg, Steen Uttrup Pedersen, Mikkel Kongsfelt, and Mie Lillethorup, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00205. keywords: {polymer brushes;surfaceinitiated controlled radical polymerization (SICRP);thin films;longlived;industrial scale} |