Surface-Enriched Amphiphilic Polysiloxane Coating with Superior Antifouling Ability and Strong Substrate Adhesion AITranslate

South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The coexistence of superior antifouling ability and strong substrate adhesion is a typical trade-off for a silicone coating but is highly desirable in numerous applications. Herein, we present a surface-enriched antifouling coating consisting of a bis-silane-terminated polyurea (SPU), an oligosiloxane nanocluster, and a bi-silanol-terminated poly(dimethylsiloxane) with fluorocarbon and poly(ethylene glycol) side chains as a reactive amphiphilic polymer (RAP). The oligosiloxane nanoclusters can cross-link the flexible SPU into a tough polymer network and interlink the polymer network to the substrate, whereas the low-surface-energy RAP can self-enrich on the surface during coating formation. Such a polysiloxane coating exhibits high transparency (>85% transmittance), high tensile strength (∼12 MPa), superior fouling resistance against proteins and bacteria, and strong adhesion strength on various substrates including glass, ceramic, steel, Ti, and epoxy (3–15 MPa). This research provides a universal and tunable approach for the future design of antifouling coatings in flexible electronics, medical devices, and marine industries.

KeyWords AITranslate

antifouling coating polysiloxane oligosiloxane nanocluster selfenriched strong adhesion
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00199

Chinese Library Classification Number:

Citation Information:

The coexistence of superior antifouling ability and strong substrate adhesion is a typical trade-off for a silicone coating but is highly desirable in numerous applications. Herein, we present a surface-enriched antifouling coating consisting of a bis-silane-terminated polyurea (SPU), an oligosiloxane nanocluster, and a bi-silanol-terminated poly(dimethylsiloxane) with fluorocarbon and poly(ethylene glycol) side chains as a reactive amphiphilic polymer (RAP). The oligosiloxane nanoclusters can cross-link the flexible SPU into a tough polymer network and interlink the polymer network to the substrate, whereas the low-surface-energy RAP can self-enrich on the surface during coating formation. Such a polysiloxane coating exhibits high transparency (>85% transmittance), high tensile strength (∼12 MPa), superior fouling resistance against proteins and bacteria, and strong adhesion strength on various substrates including glass, ceramic, steel, Ti, and epoxy (3–15 MPa). This research provides a universal and tunable approach for the future design of antifouling coatings in flexible electronics, medical devices, and marine industries.

quote

GB/T 7714-2015 [1] Zhenqiang Zhang, Qingyi Xie, Guoliang Zhang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00199.
MLA [1] Zhenqiang Zhang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00199.
APA [1] Zhenqiang Zhang, Qingyi Xie, Guoliang Zhang, Chunfeng Ma, & Guangzhao Zhang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00199
IEEE [1] Zhenqiang Zhang, Qingyi Xie, Guoliang Zhang, Chunfeng Ma, and Guangzhao Zhang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00199. keywords: {antifouling coating;polysiloxane;oligosiloxane nanocluster;selfenriched;strong adhesion}