Polyzwitterionic Nanogels for Controlled and Sustained Release of Bicarbonate Anions for Treatment of Metabolic Acidosis AITranslate

Indian Institute of Technology; Indian Institute of Technology; Indian Institute of Technology; Indian Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Despite the reported evidence of deleterious effects of metabolic acidosis (MA), the development of advanced treatment options for this critical condition has not been explored much. Based on fundamental research and clinical trials, correcting MA with bicarbonate anions has a vast array of potential benefits. To achieve this objective, herein, we report on cytocompatible, charged polyzwitterionic nanogels (PZNGs) that can efficiently fix and release bicarbonate anions by a controlled and sustained mechanism. Three different PZNGs were synthesized using free radical polymerization with Pluronic F-127 as a non-ionic surfactant. From dynamic light scattering analysis, the hydrodynamic sizes (Dh) were found to be 68 ± 6, 120 ± 3, and 97 ± 9 nm for PZNG-1, PZNG-2, and PZNG-3, respectively. The fixation of HCO3– on PZNGs was done either by direct reaction with NaHCO3 or by CO2 gas bubbling into a dispersion of PZNGs, and the maximum loading efficiency was found to be ∼87–95%. Accelerated stability studies showed good stability for 30 days at 25 and 2–8 °C for the nanogels. The cytocompatibility results of the PZNGs from the MTT assay and the live–dead test confirm their non-toxicity, safety, and potential for various biomedical applications. The in vitro drug release profile revealed a sustained and controlled release pattern of HCO3– with a maximum of ∼90% cumulative release in 168 h. The Korsmeyer–Peppas kinetic model suggests that the HCO3– anion release was regulated by diffusion of the anions and swelling of polymeric nanogels. In addition to the fixation and sustained release mechanisms described, the PZNGs reported here act as a simple and efficient carrier to deliver HCO3– anions for the treatment of MA with reduced complications.

KeyWords AITranslate

nanogel polyzwitterion bicarbonate metabolic acidosis controlled and sustained release
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00221

Chinese Library Classification Number:

Citation Information:

Despite the reported evidence of deleterious effects of metabolic acidosis (MA), the development of advanced treatment options for this critical condition has not been explored much. Based on fundamental research and clinical trials, correcting MA with bicarbonate anions has a vast array of potential benefits. To achieve this objective, herein, we report on cytocompatible, charged polyzwitterionic nanogels (PZNGs) that can efficiently fix and release bicarbonate anions by a controlled and sustained mechanism. Three different PZNGs were synthesized using free radical polymerization with Pluronic F-127 as a non-ionic surfactant. From dynamic light scattering analysis, the hydrodynamic sizes (Dh) were found to be 68 ± 6, 120 ± 3, and 97 ± 9 nm for PZNG-1, PZNG-2, and PZNG-3, respectively. The fixation of HCO3– on PZNGs was done either by direct reaction with NaHCO3 or by CO2 gas bubbling into a dispersion of PZNGs, and the maximum loading efficiency was found to be ∼87–95%. Accelerated stability studies showed good stability for 30 days at 25 and 2–8 °C for the nanogels. The cytocompatibility results of the PZNGs from the MTT assay and the live–dead test confirm their non-toxicity, safety, and potential for various biomedical applications. The in vitro drug release profile revealed a sustained and controlled release pattern of HCO3– with a maximum of ∼90% cumulative release in 168 h. The Korsmeyer–Peppas kinetic model suggests that the HCO3– anion release was regulated by diffusion of the anions and swelling of polymeric nanogels. In addition to the fixation and sustained release mechanisms described, the PZNGs reported here act as a simple and efficient carrier to deliver HCO3– anions for the treatment of MA with reduced complications.

quote

GB/T 7714-2015 [1] Ujjawal Bairagi, Simran Kaur Rainu, Neetu Singh, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00221.
MLA [1] Ujjawal Bairagi, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00221.
APA [1] Ujjawal Bairagi, Simran Kaur Rainu, Neetu Singh, & Josemon Jacob. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00221
IEEE [1] Ujjawal Bairagi, Simran Kaur Rainu, Neetu Singh, and Josemon Jacob, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00221. keywords: {nanogel;polyzwitterion;bicarbonate;metabolic acidosis;controlled and sustained release}