FACsPb Triple Halide Perovskite Solar Cells with Thermal Operation over 200 °C AITranslate

University of Oklahoma; University of Oklahoma; University of Oklahoma; University of Oklahoma; University of Oklahoma; University of North Texas;National Renewable Energy Laboratory;National Renewable Energy Laboratory;Swift Solar, San Carlos; University of Oklahoma
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Formamidinium cesium (FACs) perovskites solar cells have been shown to be among the most stable metal halide perovskites. Here, high-temperature data are presented which systematically and statistically demonstrate the high thermal operation of this system to temperatures in excess of 200 °C. Device measurements between 250 K and 490 K show that while some loss of performance is evident at higher temperature, this is driven by reversible halide segregation with no evidence of a structural phase transition over the measurement range probed. Moreover, upon reduction of the temperature back to ambient the power conversion efficiency is retained.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00551

Chinese Library Classification Number:

Citation Information:

Formamidinium cesium (FACs) perovskites solar cells have been shown to be among the most stable metal halide perovskites. Here, high-temperature data are presented which systematically and statistically demonstrate the high thermal operation of this system to temperatures in excess of 200 °C. Device measurements between 250 K and 490 K show that while some loss of performance is evident at higher temperature, this is driven by reversible halide segregation with no evidence of a structural phase transition over the measurement range probed. Moreover, upon reduction of the temperature back to ambient the power conversion efficiency is retained.

quote

GB/T 7714-2015 [1] Hadi Afshari, Shashi Sourabh, Sergio A. Chacon, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00551.
MLA [1] Hadi Afshari, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00551.
APA [1] Hadi Afshari, Shashi Sourabh, Sergio A. Chacon, Vincent R. Whiteside, Rachel C. Penner, Bibhudutta Rout, Ahmad R. Kirmani, Joseph M. Luther, Giles E. Eperon, & Ian R. Sellers. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00551