Mitigating the High-Charge Detrimental Phase Transformation in LiNiO2 Using Doping Engineering AITranslate

Lawrence Berkeley National Laboratory; Florida State University; University of California
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cobalt-free layered LiNiO2 has gained increased interest due to the scarcity and high cost of cobalt. However, LiNiO2 suffers from poor cycling stability, which is mainly due to oxygen loss and structural instability, especially when operating at high voltages. Herein, we present a doping strategy to mitigate the detrimental O3-to-O1 phase transformation in LiNiO2 from first-principles calculations. Temperature–composition phase diagrams of pristine and doped Li1–xNiO2 are obtained using a cluster-expansion and Monte Carlo simulation approach. We investigate the effects of dopant oxidation states, sizes, and concentrations on the dopant distribution in LiNi1–yMyO2 (M = Sb, Ti, Si, Al, and Mg) as well as the phase transitions during delithiation. We find that introducing high-valence dopants with ionic radii similar to that of Ni3+ into LiNiO2 stabilizes the O3-phase cathode bulk structure at high charge. Our results provide a general guidance on using doping engineering to realize Ni-rich, Co-free cathodes for lithium-ion batteries.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00169

Chinese Library Classification Number:

Citation Information:

Cobalt-free layered LiNiO2 has gained increased interest due to the scarcity and high cost of cobalt. However, LiNiO2 suffers from poor cycling stability, which is mainly due to oxygen loss and structural instability, especially when operating at high voltages. Herein, we present a doping strategy to mitigate the detrimental O3-to-O1 phase transformation in LiNiO2 from first-principles calculations. Temperature–composition phase diagrams of pristine and doped Li1–xNiO2 are obtained using a cluster-expansion and Monte Carlo simulation approach. We investigate the effects of dopant oxidation states, sizes, and concentrations on the dopant distribution in LiNi1–yMyO2 (M = Sb, Ti, Si, Al, and Mg) as well as the phase transitions during delithiation. We find that introducing high-valence dopants with ionic radii similar to that of Ni3+ into LiNiO2 stabilizes the O3-phase cathode bulk structure at high charge. Our results provide a general guidance on using doping engineering to realize Ni-rich, Co-free cathodes for lithium-ion batteries.

quote

GB/T 7714-2015 [1] Jianli Cheng, Bin Ouyang, Kristin A. Persson. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00169.
MLA [1] Jianli Cheng, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00169.
APA [1] Jianli Cheng, Bin Ouyang, & Kristin A. Persson. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00169
IEEE [1] Jianli Cheng, Bin Ouyang, and Kristin A. Persson, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00169.