daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

UV Encapsulated Monolithic Perovskite/Silicon Tandem Solar Cells for Hundred-Watt Power System AITranslate

Shihezi University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University; Nankai University;Gold Stone (Fujian) Energy Company Ltd.;Gold Stone (Fujian) Energy Company Ltd.; Nankai University; Nankai University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Efficient and lossless encapsulation must be resolved before the industrialization of monolithic perovskite/silicon tandem solar cells (PSTs). Here, an ultraviolet (UV) curable material, which is environmentally friendly and needs only 1 min of UV solidification, is designed and used to encapsulate three types of typical PSTs, namely, flat structure, special texture structure, and commercial texture structure. Since the cured encapsulating material has an appropriate refractive index similar to glass and has a nondestructive impact on the perovskite, the performance of encapsulated devices improves with the increase of current density. The device stability tests (including immersion in water and weak acid, outdoor exposure, −35°C, and 60°C/85RH% environment) demonstrated an initial efficiency of more than 90% after 1000 h. A 100 W PST power station is built by encapsulating PSTs with an expanded area (>10 cm2).

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00275

Chinese Library Classification Number:

Citation Information:

Efficient and lossless encapsulation must be resolved before the industrialization of monolithic perovskite/silicon tandem solar cells (PSTs). Here, an ultraviolet (UV) curable material, which is environmentally friendly and needs only 1 min of UV solidification, is designed and used to encapsulate three types of typical PSTs, namely, flat structure, special texture structure, and commercial texture structure. Since the cured encapsulating material has an appropriate refractive index similar to glass and has a nondestructive impact on the perovskite, the performance of encapsulated devices improves with the increase of current density. The device stability tests (including immersion in water and weak acid, outdoor exposure, −35°C, and 60°C/85RH% environment) demonstrated an initial efficiency of more than 90% after 1000 h. A 100 W PST power station is built by encapsulating PSTs with an expanded area (>10 cm2).

quote

GB/T 7714-2015 [1] Renjie Li, Qiaojing Xu, Biao Shi, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00275.
MLA [1] Renjie Li, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00275.
APA [1] Renjie Li, Qiaojing Xu, Biao Shi, Jin Wang, Yucheng Li, Bingbing Chen, Jingjing Liu, Ningyu Ren, Wei Han, Yuxiang Li, Cong Sun, Zhao Zhu, Yubo Zhang, Pengfei Liu, Xiaojing Han, Jing Dong, Xuejiao Wang, Zixuan Huang, Youkang Gong, . . . Xiaodan Zhang. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00275
IEEE [1] Renjie Li, Qiaojing Xu, Biao Shi, Jin Wang, Yucheng Li, Bingbing Chen, Jingjing Liu, Ningyu Ren, Wei Han, Yuxiang Li, Cong Sun, Zhao Zhu, Yubo Zhang, Pengfei Liu, Xiaojing Han, Jing Dong, Xuejiao Wang, Zixuan Huang, Youkang Gong, Shengzhi Xu, Pengyang Wang, Qian Huang, Dekun Zhang, Xiaona Du, Huizhi Ren, Chaohua Zhang, Huihu Zhuang, Ying Zhao, and Xiaodan Zhang, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00275.