daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

The effects of electrically-assisted ultrasonic nanocrystal surface modification on 3D-printed Ti-6Al-4V alloy AITranslate

The University of Akron; The University of Akron; The University of Akron; The University of Akron; The University of Akron; The University of Akron; The University of Akron; The University of Akron
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

3D-printed Ti-6Al-4V components have great potential in the aerospace and biomedical industries. However, their wide application is limited by some inherent disadvantages, such as poor surface finish and high porosity. In this study, an innovative method, electrically-assisted ultrasonic nanocrystal surface modification (EA-UNSM) was introduced to process 3D-printed Ti-6Al-4V samples. The effect of EA-UNSM on surface finish, microstructure, porosity and in-depth hardness was investigated. Compared with the conventional UNSM process, smoother surfaces and lower subsurface porosities were obtained after EA-UNSM. EA-UNSM also led to a thicker plastically-affected depth compared with conventional UNSM. Numerical modelling showed that localized heating occurs near the pores in 3D-printed Ti-6Al-4V subjected to electric current. This localized heating could potentially facilitate pore closure under ultrasonic striking.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.addma.2018.04.035

Chinese Library Classification Number:

Citation Information:

3D-printed Ti-6Al-4V components have great potential in the aerospace and biomedical industries. However, their wide application is limited by some inherent disadvantages, such as poor surface finish and high porosity. In this study, an innovative method, electrically-assisted ultrasonic nanocrystal surface modification (EA-UNSM) was introduced to process 3D-printed Ti-6Al-4V samples. The effect of EA-UNSM on surface finish, microstructure, porosity and in-depth hardness was investigated. Compared with the conventional UNSM process, smoother surfaces and lower subsurface porosities were obtained after EA-UNSM. EA-UNSM also led to a thicker plastically-affected depth compared with conventional UNSM. Numerical modelling showed that localized heating occurs near the pores in 3D-printed Ti-6Al-4V subjected to electric current. This localized heating could potentially facilitate pore closure under ultrasonic striking.

quote

GB/T 7714-2015 [1] Hao Zhang, Jingyi Zhao, Jun Liu, et al. Additive Manufacturing, 2018(22). DOI:10.1016/j.addma.2018.04.035.
MLA [1] Hao Zhang, et al., Additive Manufacturing, no. 22, 2018, https://doi.org/10.1016/j.addma.2018.04.035.
APA [1] Hao Zhang, Jingyi Zhao, Jun Liu, Haifeng Qin, Zhencheng Ren, G.L. Doll, Yalin Dong, & Chang Ye. (2018). Additive Manufacturing(22). https://doi.org/10.1016/j.addma.2018.04.035
IEEE [1] Hao Zhang, Jingyi Zhao, Jun Liu, Haifeng Qin, Zhencheng Ren, G.L. Doll, Yalin Dong, and Chang Ye, Additive Manufacturing, no. 22, 2018, doi: 10.1016/j.addma.2018.04.035.