Fused filament fabrication melting model AITranslate

University of Wisconsin–Madison; University of Wisconsin–Madison;Friedrich Alexander University–Erlangen
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This paper presents an analytical melting model inside the nozzle of a fused filament fabrication process. The model presents the limiting case scenario where the maximum melting rate is controlled by the applied force. Here, instead of having a nozzle filled with polymer melt, the melt is reduced to a melt film at the tip of the filament as it is pushed against the exit of the nozzle. The model uses a mode of melting that is governed by melting with pressure flow melt removal. The model includes effects of initial filament temperatures, heater temperature, applied force, nozzle tip angle, capillary diameter and length as well as rheological and thermal properties. The analytical solution is compared to controlled experiments done on a specially designed set-up. Furthermore, the model is used to assess the effect of nozzle tip angle, heater temperature and initial filament temperature on the melting rate within the nozzle. The comparison between the experiments and the model show that assumptions used for the model development are plausible, and that the model can be used to optimize the melting within a material extrusion additive manufacturing process, as well as predicting the performance of new materials.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.addma.2018.04.030

Chinese Library Classification Number:

Citation Information:

This paper presents an analytical melting model inside the nozzle of a fused filament fabrication process. The model presents the limiting case scenario where the maximum melting rate is controlled by the applied force. Here, instead of having a nozzle filled with polymer melt, the melt is reduced to a melt film at the tip of the filament as it is pushed against the exit of the nozzle. The model uses a mode of melting that is governed by melting with pressure flow melt removal. The model includes effects of initial filament temperatures, heater temperature, applied force, nozzle tip angle, capillary diameter and length as well as rheological and thermal properties. The analytical solution is compared to controlled experiments done on a specially designed set-up. Furthermore, the model is used to assess the effect of nozzle tip angle, heater temperature and initial filament temperature on the melting rate within the nozzle. The comparison between the experiments and the model show that assumptions used for the model development are plausible, and that the model can be used to optimize the melting within a material extrusion additive manufacturing process, as well as predicting the performance of new materials.

quote

GB/T 7714-2015 [1] Tim A. Osswald, John Puentes, Julian Kattinger. Additive Manufacturing, 2018(22). DOI:10.1016/j.addma.2018.04.030.
MLA [1] Tim A. Osswald, et al., Additive Manufacturing, no. 22, 2018, https://doi.org/10.1016/j.addma.2018.04.030.
APA [1] Tim A. Osswald, John Puentes, & Julian Kattinger. (2018). Additive Manufacturing(22). https://doi.org/10.1016/j.addma.2018.04.030
IEEE [1] Tim A. Osswald, John Puentes, and Julian Kattinger, Additive Manufacturing, no. 22, 2018, doi: 10.1016/j.addma.2018.04.030.