daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Bio-Based Tannin-Furanic-Silk Adhesives: Applications in Plywood and Chemical Cross-linking Mechanisms AITranslate

University of Padua; Salzburg University of Applied Sciences; University of Perugia; University of Perugia; National Institute of Chemistry; University of Padua;Elettra Sincrotrone Triete, S.S.14 Km
1
6
3.5 in Area Science Prk; University of Padua; University of Padua
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Wood polyphenolic extracts, commonly called tannins, are excellent candidates for the production of bioplastics due to their abundance in nature, their commercial availability, and their reactivity. In particular, they were tested as wood adhesives with several hardeners, but their low moisture resistance and their rigidity reduced their technological interest. In the present study, we combined regenerated silk (RS) with tannin-furanic formulations to improve their properties. Three-layer plywood glued with these several fully renewable tannin-silk-furanic adhesives were tested for their mechanical properties: the modulus of elasticity, the modulus of rupture, and both dry and wet shear strength were enhanced when 20 wt % of RS was added. Initially, the cross section of the prepared samples was investigated by scanning electron microscopy, indicating a good dispersion of RS within the tannin-furanic matrix. Afterward, thermomechanical analysis of the adhesive highlighted that RS slows down the polymerization rate, decreasing the cross-linking kinetics of polyfurfuryl alcohol. Chemical investigations through ATR-FTIR and 13C-NMR show the formation of covalent bonds between RS and the furanic matrix. In summary, the combination of bioresources from the vegetal and animal kingdom allows the manufacturing of fully bio-based adhesives with enhanced mechanical properties and water resistance. This represents an important breakthrough in the exploitation of polyphenols, opening perspectives for their application in material science.

KeyWords AITranslate

regenerated silk protein fibroin flavonoids furanic engineered wood products sustainable
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00539

Chinese Library Classification Number:

Citation Information:

Wood polyphenolic extracts, commonly called tannins, are excellent candidates for the production of bioplastics due to their abundance in nature, their commercial availability, and their reactivity. In particular, they were tested as wood adhesives with several hardeners, but their low moisture resistance and their rigidity reduced their technological interest. In the present study, we combined regenerated silk (RS) with tannin-furanic formulations to improve their properties. Three-layer plywood glued with these several fully renewable tannin-silk-furanic adhesives were tested for their mechanical properties: the modulus of elasticity, the modulus of rupture, and both dry and wet shear strength were enhanced when 20 wt % of RS was added. Initially, the cross section of the prepared samples was investigated by scanning electron microscopy, indicating a good dispersion of RS within the tannin-furanic matrix. Afterward, thermomechanical analysis of the adhesive highlighted that RS slows down the polymerization rate, decreasing the cross-linking kinetics of polyfurfuryl alcohol. Chemical investigations through ATR-FTIR and 13C-NMR show the formation of covalent bonds between RS and the furanic matrix. In summary, the combination of bioresources from the vegetal and animal kingdom allows the manufacturing of fully bio-based adhesives with enhanced mechanical properties and water resistance. This represents an important breakthrough in the exploitation of polyphenols, opening perspectives for their application in material science.

quote

GB/T 7714-2015 [1] Emanuele Cesprini, Johannes Jorda, Marco Paolantoni, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00539.
MLA [1] Emanuele Cesprini, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00539.
APA [1] Emanuele Cesprini, Johannes Jorda, Marco Paolantoni, Luca Valentini, Primož Šket, Valerio Causin, Diana E. Bedolla, Michela Zanetti, & Gianluca Tondi. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00539
IEEE [1] Emanuele Cesprini, Johannes Jorda, Marco Paolantoni, Luca Valentini, Primož Šket, Valerio Causin, Diana E. Bedolla, Michela Zanetti, and Gianluca Tondi, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00539. keywords: {regenerated silk;protein;fibroin;flavonoids;furanic;engineered wood products;sustainable}