daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Capacitive/Resistive Strain Sensors Based on Organogel/Hydrogel Hybrids via a Low-Swelling Solvent Replacement Strategy AITranslate

University of Science and Technology of China; University of Science and Technology of China; University of Science and Technology of China; University of Science and Technology of China; University of Science and Technology of China; University of Science and Technology of China; University of Science and Technology of China
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

As potential flexible sensors to mimic skin functions or achieve human–computer interactions, organogel/hydrogel hybrids, prepared mostly through “adhesion strategies” and “interfacial polymerization strategies”, have gained increasing attention in recent years. Herein, the organogel/hydrogel hybrids with different structures and functions were prepared through a low-swelling solvent replacement strategy. Organogel/hydrogel hybrids were prepared by in situ solvent replacement with aqueous NaCl solution (10 wt %) on native organogels, which were fabricated by photoinitiated copolymerization of methacrylic acid (MAAc) and N-(pyridin-2-yl)acrylamide (NPAM) in glycerol. Capacitive or resistive modal sensors based on organogel/hydrogel hybrids can be obtained easily. In particular, because the patterns were completely dependent on the mold containing the displacing solvent, flexible electronic sensors based on organogel/hydrogel hybrids with complex topological structures and functions could be designed and prepared conveniently. Since the interface between the hydrogel and the organogel also formed in situ and was very strong, the organogel/hydrogel hybrids exhibit excellent puncture-resistant performance. Our experimental results indicated that organogel/hydrogel hybrids with complex patterns and topologies could be prepared through a low-swelling solvent replacement strategy. The design and practical application of flexible electronic sensors based on organogel/hydrogel hybrids will be enlarged and advanced substantially.

KeyWords AITranslate

capacitive sensors resistive sensors organogel/hydrogel hybrids solvent replacement punctureresistant
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00610

Chinese Library Classification Number:

Citation Information:

As potential flexible sensors to mimic skin functions or achieve human–computer interactions, organogel/hydrogel hybrids, prepared mostly through “adhesion strategies” and “interfacial polymerization strategies”, have gained increasing attention in recent years. Herein, the organogel/hydrogel hybrids with different structures and functions were prepared through a low-swelling solvent replacement strategy. Organogel/hydrogel hybrids were prepared by in situ solvent replacement with aqueous NaCl solution (10 wt %) on native organogels, which were fabricated by photoinitiated copolymerization of methacrylic acid (MAAc) and N-(pyridin-2-yl)acrylamide (NPAM) in glycerol. Capacitive or resistive modal sensors based on organogel/hydrogel hybrids can be obtained easily. In particular, because the patterns were completely dependent on the mold containing the displacing solvent, flexible electronic sensors based on organogel/hydrogel hybrids with complex topological structures and functions could be designed and prepared conveniently. Since the interface between the hydrogel and the organogel also formed in situ and was very strong, the organogel/hydrogel hybrids exhibit excellent puncture-resistant performance. Our experimental results indicated that organogel/hydrogel hybrids with complex patterns and topologies could be prepared through a low-swelling solvent replacement strategy. The design and practical application of flexible electronic sensors based on organogel/hydrogel hybrids will be enlarged and advanced substantially.

quote

GB/T 7714-2015 [1] Qiang Zhou, Jiaqing He, Zhiqing Ge, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00610.
MLA [1] Qiang Zhou, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00610.
APA [1] Qiang Zhou, Jiaqing He, Zhiqing Ge, Chao Xu, Kaixiang Yang, Gang Zou, & Haiyang Yang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00610
IEEE [1] Qiang Zhou, Jiaqing He, Zhiqing Ge, Chao Xu, Kaixiang Yang, Gang Zou, and Haiyang Yang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00610. keywords: {capacitive sensors;resistive sensors;organogel/hydrogel hybrids;solvent replacement;punctureresistant}