daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Synthesis of a Reactive Oxygen Species Responsive Star Polymer for the Controlled Release of Carbendazim AITranslate

Shihezi University/Key Laboratory for Green Processing of Chemical Engineering of Xinjiang Bingtuan/Key Laboratory of Materials-Oriented Chemical Engineering of Xinjiang Uygur Autonomous Region/Engineering Research Center of Materials-Oriented Chemical Engineering of Xinjiang Bingtuan; Shihezi University/Key Laboratory for Green Processing of Chemical Engineering of Xinjiang Bingtuan/Key Laboratory of Materials-Oriented Chemical Engineering of Xinjiang Uygur Autonomous Region/Engineering Research Center of Materials-Oriented Chemical Engineering of Xinjiang Bingtuan; Shihezi University/Key Laboratory for Green Processing of Chemical Engineering of Xinjiang Bingtuan/Key Laboratory of Materials-Oriented Chemical Engineering of Xinjiang Uygur Autonomous Region/Engineering Research Center of Materials-Oriented Chemical Engineering of Xinjiang Bingtuan; Shihezi University/Key Laboratory for Green Processing of Chemical Engineering of Xinjiang Bingtuan/Key Laboratory of Materials-Oriented Chemical Engineering of Xinjiang Uygur Autonomous Region/Engineering Research Center of Materials-Oriented Chemical Engineering of Xinjiang Bingtuan; Shihezi University; Shihezi University/Key Laboratory for Green Processing of Chemical Engineering of Xinjiang Bingtuan/Key Laboratory of Materials-Oriented Chemical Engineering of Xinjiang Uygur Autonomous Region/Engineering Research Center of Materials-Oriented Chemical Engineering of Xinjiang Bingtuan; Shihezi University/Key Laboratory for Green Processing of Chemical Engineering of Xinjiang Bingtuan/Key Laboratory of Materials-Oriented Chemical Engineering of Xinjiang Uygur Autonomous Region/Engineering Research Center of Materials-Oriented Chemical Engineering of Xinjiang Bingtuan; East China University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

An intelligent responsive pesticide delivery system has been applied in agriculture to improve the utilization rate of pesticides. When plants are affected by fungi, a large number of reactive oxygen species (ROS) are produced rapidly on the wound surface. Based on this, a ROS responsive star polymer micellar slow-release system was constructed to load carbendazim (MBC) and improve its bioavailability. The star polymer was synthesized by using 3-mercaptopropionic acid, acetone, pentaerythritol (PER), ε-caprolactone (ε-CL), and methoxypolyethylene glycols (mPEG5000, Mw = 5000) and named PER-PCL-TK-mPEG5000. By loading MBC, the drug loading micelle MBC-loaded PER-PCL-TK-mPEG5000 was obtained. The cumulative release amount of MBC-loaded PER-PCL-TK-mPEG5000 containing H2O2 is 1.64 times of that without H2O2 after 120 h release. The inhibitory rate of MBC-loaded PER-PCL-TK-mPEG5000 containing H2O2 against Rhizoctonia solani (R. solani) was 91.6%. The critical micelle concentration (CMC) of PER-PCL-TK-mPEG5000 is 4.37 mg/L, and the result showed that PER-PCL-TK-mPEG5000 and MBC-loaded PER-PCL-TK-mPEG5000 have good stability at 4 °C for 14 d. This study proved that the strategy of designing pesticide vectors according to the target environment can be widely used to protect crops, improve pesticide utilization rate, and protect the environment.

KeyWords AITranslate

star polymer ROS responsive carbendazim controlled release antibacterial properties
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00603

Chinese Library Classification Number:

Citation Information:

An intelligent responsive pesticide delivery system has been applied in agriculture to improve the utilization rate of pesticides. When plants are affected by fungi, a large number of reactive oxygen species (ROS) are produced rapidly on the wound surface. Based on this, a ROS responsive star polymer micellar slow-release system was constructed to load carbendazim (MBC) and improve its bioavailability. The star polymer was synthesized by using 3-mercaptopropionic acid, acetone, pentaerythritol (PER), ε-caprolactone (ε-CL), and methoxypolyethylene glycols (mPEG5000, Mw = 5000) and named PER-PCL-TK-mPEG5000. By loading MBC, the drug loading micelle MBC-loaded PER-PCL-TK-mPEG5000 was obtained. The cumulative release amount of MBC-loaded PER-PCL-TK-mPEG5000 containing H2O2 is 1.64 times of that without H2O2 after 120 h release. The inhibitory rate of MBC-loaded PER-PCL-TK-mPEG5000 containing H2O2 against Rhizoctonia solani (R. solani) was 91.6%. The critical micelle concentration (CMC) of PER-PCL-TK-mPEG5000 is 4.37 mg/L, and the result showed that PER-PCL-TK-mPEG5000 and MBC-loaded PER-PCL-TK-mPEG5000 have good stability at 4 °C for 14 d. This study proved that the strategy of designing pesticide vectors according to the target environment can be widely used to protect crops, improve pesticide utilization rate, and protect the environment.

quote

GB/T 7714-2015 [1] Yan Qin, Weihua Su, Guihua Meng, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00603.
MLA [1] Yan Qin, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00603.
APA [1] Yan Qin, Weihua Su, Guihua Meng, Jianning Wu, Lin Cui, Shengchao Yang, Zhiyong Liu, & Xuhong Guo. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00603