daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Compositionally Screened Eutectic Catalytic Coatings on Halide Perovskite Photocathodes for Photoassisted Selective CO2 Reduction AITranslate

King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Selective CO2 reduction via photoelectrocatalysis is a creative approach to alleviating the energy crisis and environmental deterioration as well as to producing value-added chemicals. A considerable challenge is the development of electrocatalysts and photoelectrocatalytic systems to selectively and efficiently produce a target product. Here, we report an efficient and selective photocathode for converting CO2 to HCOOH in aqueous solution. A rational compositional screening strategy was first applied to pinpoint In0.4Bi0.6 from ternary In–Bi–Sn alloys as the most HCOOH-selective electrocatalyst composition among the electrocatalysts reported. A photocathode was then fabricated by coating the catalytic, protective, and conductive In0.4Bi0.6 alloy layer on a halide perovskite photovoltaic, effectively utilizing its low melting point eutectic molten state. The generated photovoltage assisted reduction of the overpotential by 680 mV while producing a stable current for nearly exclusive HCOOH production under simulated AM 1.5G irradiation. This work provides a promising approach to achieving efficient and selective solar–fuel conversion.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b00751

Chinese Library Classification Number:

Citation Information:

Selective CO2 reduction via photoelectrocatalysis is a creative approach to alleviating the energy crisis and environmental deterioration as well as to producing value-added chemicals. A considerable challenge is the development of electrocatalysts and photoelectrocatalytic systems to selectively and efficiently produce a target product. Here, we report an efficient and selective photocathode for converting CO2 to HCOOH in aqueous solution. A rational compositional screening strategy was first applied to pinpoint In0.4Bi0.6 from ternary In–Bi–Sn alloys as the most HCOOH-selective electrocatalyst composition among the electrocatalysts reported. A photocathode was then fabricated by coating the catalytic, protective, and conductive In0.4Bi0.6 alloy layer on a halide perovskite photovoltaic, effectively utilizing its low melting point eutectic molten state. The generated photovoltage assisted reduction of the overpotential by 680 mV while producing a stable current for nearly exclusive HCOOH production under simulated AM 1.5G irradiation. This work provides a promising approach to achieving efficient and selective solar–fuel conversion.

quote

GB/T 7714-2015 [1] Jie Chen, Jun Yin, Xiaopeng Zheng, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00751.
MLA [1] Jie Chen, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00751.
APA [1] Jie Chen, Jun Yin, Xiaopeng Zheng, Hassan Ait Ahsaine, Yang Zhou, Chunwei Dong, Omar F. Mohammed, Kazuhiro Takanabe, & Osman M. Bakr. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00751
IEEE [1] Jie Chen, Jun Yin, Xiaopeng Zheng, Hassan Ait Ahsaine, Yang Zhou, Chunwei Dong, Omar F. Mohammed, Kazuhiro Takanabe, and Osman M. Bakr, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00751.