Abstract AITranslate

The practical application of rechargeable lithium (Li) metal batteries has long been hindered by the unstable Li metal anode with problems like Li dendrite growth, low Coulombic efficiency (CE), and short cycle life. Here, we demonstrate a multifunctional sulfur-containing hybrid Li polysulfidophosphate and poly(2-chloroethyl acrylate) cross-linking film that can provide effective protection for Li metal anode. This film can facilitate Li metal anode generating a stable organic/inorganic hybrid solid electrolyte interphase (SEI) layer containing multiple components such as polymer-tethered organo(poly)sulfide, inorganic Li polysulfidophosphate, Li sulfides, and Li salts. Thanks to this hybrid robust SEI layer, dendrite-free Li deposition and stable cycling of Li metal anode can be achieved (e.g., CE > 98.7% over 950 cycles). We demonstrated this Li protection technique enables both the protected Li metal anode and Li-metal-free anode cycling with significantly improved CEs and stability in full cells using LiFePO4 (∼2.4 mAh/cm2) cathode.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b00539

Chinese Library Classification Number:

Citation Information:

The practical application of rechargeable lithium (Li) metal batteries has long been hindered by the unstable Li metal anode with problems like Li dendrite growth, low Coulombic efficiency (CE), and short cycle life. Here, we demonstrate a multifunctional sulfur-containing hybrid Li polysulfidophosphate and poly(2-chloroethyl acrylate) cross-linking film that can provide effective protection for Li metal anode. This film can facilitate Li metal anode generating a stable organic/inorganic hybrid solid electrolyte interphase (SEI) layer containing multiple components such as polymer-tethered organo(poly)sulfide, inorganic Li polysulfidophosphate, Li sulfides, and Li salts. Thanks to this hybrid robust SEI layer, dendrite-free Li deposition and stable cycling of Li metal anode can be achieved (e.g., CE > 98.7% over 950 cycles). We demonstrated this Li protection technique enables both the protected Li metal anode and Li-metal-free anode cycling with significantly improved CEs and stability in full cells using LiFePO4 (∼2.4 mAh/cm2) cathode.

quote

GB/T 7714-2015 [1] Yuming Zhao, Guoxing Li, Yue Gao, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00539.
MLA [1] Yuming Zhao, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00539.
APA [1] Yuming Zhao, Guoxing Li, Yue Gao, Daiwei Wang, Qingquan Huang, & Donghai Wang. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00539
IEEE [1] Yuming Zhao, Guoxing Li, Yue Gao, Daiwei Wang, Qingquan Huang, and Donghai Wang, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00539.