Highly Active and Stable Water Splitting in Acidic Media Using a Bifunctional Iridium/Cucurbit[6]uril Catalyst AITranslate
Abstract AITranslate
Water electrolysis offers an ideal process for generating hydrogen, the most promising form of clean energy. Splitting water in acidic media has had limited progress to date because of the low anodic oxygen evolution reaction activity and serious catalyst degradation. Here, we report a bifunctional Ir catalyst stabilized by cucurbit[6]uril for water splitting in acidic media. We achieved a 10 mA/cm2 overall water-splitting current density at only 1.56 V, which is among the highest activities reported. Moreover, our cell showed a high stability of at least 20 h of continuous operation at 5 mA/cm2. Spectroscopic experiments and theoretical calculations revealed that the coordination interaction between Ir atoms and cucurbit[6]uril facilitates the controllable synthesis and stabilization of surface active IrOx species, which leads to the excellent catalytic activity and stability observed.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.9b00553
Chinese Library Classification Number:
Citation Information:
Water electrolysis offers an ideal process for generating hydrogen, the most promising form of clean energy. Splitting water in acidic media has had limited progress to date because of the low anodic oxygen evolution reaction activity and serious catalyst degradation. Here, we report a bifunctional Ir catalyst stabilized by cucurbit[6]uril for water splitting in acidic media. We achieved a 10 mA/cm2 overall water-splitting current density at only 1.56 V, which is among the highest activities reported. Moreover, our cell showed a high stability of at least 20 h of continuous operation at 5 mA/cm2. Spectroscopic experiments and theoretical calculations revealed that the coordination interaction between Ir atoms and cucurbit[6]uril facilitates the controllable synthesis and stabilization of surface active IrOx species, which leads to the excellent catalytic activity and stability observed.
quote
| GB/T 7714-2015 | [1] Hanhui You, Dongshuang Wu, Zhening Chen, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00553. |
| MLA | [1] Hanhui You, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00553. |
| APA | [1] Hanhui You, Dongshuang Wu, Zhening Chen, Fanfei Sun, Hao Zhang, Zhenhua Chen, Minna Cao, Wei Zhuang, & Rong Cao. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00553 |
| IEEE | [1] Hanhui You, Dongshuang Wu, Zhening Chen, Fanfei Sun, Hao Zhang, Zhenhua Chen, Minna Cao, Wei Zhuang, and Rong Cao, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00553. |